Quote: Originally posted by bbartlog  
Quote:
or even try with aluminium powder


That won't work; you will get sodium aluminate, to wit:

2Al + 2NaOH + 2H2O → 2NaAlO2 + 3H2

Magnesium however will do the job.


you never heard Aluminotermia
I know Al react making aluminate but not if is dry and you
make to burn it not water at all
View user's profile View All Posts By User
verode
Harmless
*




Posts: 32
Registered: 22-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2010 at 10:42


you make Al burn with Mg burning or with glicerine and KMnO4
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 15-11-2010 at 10:49


Quote:
you never heard Aluminotermia

Nope! Any relation to thermite?

View user's profile View All Posts By User
verode
Harmless
*




Posts: 32
Registered: 22-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2010 at 11:08


Quote: Originally posted by hissingnoise  
Quote:
you never heard Aluminotermia

Nope! Any relation to thermite?

the same
View user's profile View All Posts By User
verode
Harmless
*




Posts: 32
Registered: 22-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2010 at 11:10


yes you must see
http://www.youtube.com/watch?v=i5IjDyyqIZE
View user's profile View All Posts By User
verode
Harmless
*




Posts: 32
Registered: 22-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2010 at 11:11


Quote: Originally posted by verode  
yes you must see
http://www.youtube.com/watch?v=i5IjDyyqIZE

it's very very hot
View user's profile View All Posts By User
verode
Harmless
*




Posts: 32
Registered: 22-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2010 at 11:12


yu may also try with NaF and Al or Mg but it's more difficult
Sorry my english
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2010 at 05:35


All the aluminothermic and magnesiothermic attempts at making ‘chemical sodium’ that I’ve seen (and that’s quite a few) are half-failures at best. One obtains a mixture of little sodium with a lot of slag which has proven inseparable up to and including now. At best you’ll have a few grains of contaminated sodium that do indeed test positive with water…

If you do want to successfully make gram amounts of quite pure sodium metal, melt a good dollop of NaOH in a heat resistant ceramic (or even glass) bowl, stick some graphite or steel electrodes in the melt and run a current of 5 – 10 A through it. Small globules of molten sodium will metal appear at the cathode, which can be scooped up with a gauze (steel) wire ‘spoon’ and dropped into light mineral oil where they will settle and solidify for later use. If you want to go all sophisticated use an argon or CO2 blanket to cover the ‘cell’ (and protect the sodium).

This is how Davy discovered the metal in 1807 (minus the Ar or CO2 – I saw a facsimile of the used apparatus at the British Museum, it was extraordinarily primitive) and what’s good for him should be good enough for us! ;)Alternatively build len1’s Castner Cell…
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2010 at 05:43


Quote: Originally posted by verode  
yu may also try with NaF and Al or Mg but it's more difficult
Sorry my english


In the case of 2 NaF + Mg --> 2 Na + MgF2 the reaction is likely to run so hot (heat of reaction) that the formed sodium will evaporate (well, 'zapped off' is probably a better term): sodium's BP is only 883 C. This would therefore have to carried out in a bomb reactor...
View user's profile View All Posts By User
 Pages:  1  2

  Go To Top