4N,3N,2N gallium
on one website, it says these all are 99.99 pure. so my question, stupid as it may be, is:
if the N stands for NORMALTY, what is the difference if the purity is the same.
thanks in advaNCE.
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
2N = 99%, 'N' = "nines". If it's actually 99.99%, they slipped up...is it cheaper?
If it were normality, I wonder what it would be diluted by! Gallium is 5.91 g/cm^3 and 69.723 g/mol,
http://www.google.com/search?q=5.91+g%2Fcm^3+%2F+69.723+g%2F...
84.7M. So whatever it's diluted by, 2 Normal would be about 2.5% (depending on how many bonds you count gallium's normality as).
Tim
|
|
chemrox
International Hazard
   
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
2N should be 99.99% purity and 3N should be 99.999%@12AX7; I can't get anything else out of it. Why didn't you link us to the page?
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
Fleaker
International Hazard
   
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
No. 2N is 99%, 3N5 is 99.95%, and 6N is 99.9999%.
People seem to have a gallium fixation these days :-0
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
thereelstory
Harmless
Posts: 41
Registered: 18-1-2010
Member Is Offline
Mood: No Mood
|
|
thanks, todos.
|
|
JohnWW
International Hazard
   
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
What would the impurities in Ga metal be? Most likely Al, because most Ga produced is obtained as a by-product of the refining by alkaline dissolution
of bauxite into pure alumina.
|
|