[*] posted on 11-3-2004 at 17:13
Crystalline KNO3


I took a couple pics of some crystalline KNO3 I have been fooling with. What do you guys think of this pic.

Imga0139.jpg - 76kB
View user's profile View All Posts By User This user has MSN Messenger
axehandle
Free Radical
*****




Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline

Mood: horny

[*] posted on 11-3-2004 at 17:19
Awesome!


How did you grow them?



My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35

\"Verbing nouns weirds the language!\"
View user's profile View All Posts By User
tom haggen
Hazard to Others
***




Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline

Mood: a better mood

[*] posted on 11-3-2004 at 17:31


I didn't really grow them. I just extracted them from some smoke bombs and just let them cool in that dish and got a really cool crystal formation. I figured I would post the pic.



N/A
View user's profile View All Posts By User This user has MSN Messenger
Haggis
Hazard to Others
***




Posts: 238
Registered: 1-12-2002
Location: Mid-America.
Member Is Offline

Mood: Lacrymating

[*] posted on 11-3-2004 at 18:03


Looks like they're still a bit wet. Let me guess: you let it evaporate slowly. I've found that heating crystals don't get that nice of structure.

Does your camera have a macro mode? I like to use that when I'm taking closeups of something that I want detail in. It makes it look nice.

This is a picture of some picrates being formed that I took using macro mode.

102_0285.JPG - 123kB




Great ideas often receive violent opposition from mediocre minds.
<b> <a href=\"http://pgp.mit.edu:11371/pks/lookup?op=get&search=0xEE41A2B1\">PGP Key</a> </b> 0C0A 7486 B97F 92EE AE50 A98C A4F3 087E 8CE9 A782
View user's profile View All Posts By User This user has MSN Messenger
T_FLeX
Harmless
*




Posts: 36
Registered: 31-10-2003
Location: Dirty South
Member Is Offline

Mood: Stressed

[*] posted on 11-3-2004 at 19:04


Thats pretty cool man, never seen kno3 crystals that long. The other day I made some cool looking epson salt crystals almost as long, whish I had taken some pics.



View user's profile Visit user's homepage View All Posts By User
chloric1
International Hazard
*****




Posts: 1146
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 11-3-2004 at 19:37
Crystals.


Actually, I had a few ml of 35% HNO3 left over from preparing silver nitrate from coin blanks. So instead of polluting, I neutralized it with potassium carbonate because I could. After it stopped fizzing it was about 60 degrees C. I let this set outside for a few minutes(0 degrees) and when it cooled I had lots of pretty long shards! Also, if you can get 35% perchloric acid put some roofing nails in it and wait three days. Filter and pour the blue green liquid into a large shallow dish in a warm place protected from settling dust. You should end up with some blue green ferrous perchlorate in long beautiful needles!

P.S. Most perchlorates crystalize in needle shaped crystals if the salt is sufficiently water soluble.

[Edited on 3/12/2004 by chloric1]

[Edited on 3/12/2004 by chloric1]




Fellow molecular manipulator
View user's profile View All Posts By User
tom haggen
Hazard to Others
***




Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline

Mood: a better mood

[*] posted on 11-3-2004 at 21:02


haggis, I'm not sure if I have a macro mode. is macro mode kind of like a manual focus option? I was just messing around with the manual focus option on my camera and it seems to be working much better for close ups. your pic looks extremely clear. chloric i don't really have any perchloric acid handy, though it would be nice if I did.


[Edited on 12-3-2004 by tom haggen]




N/A
View user's profile View All Posts By User This user has MSN Messenger
BromicAcid
International Hazard
*****




Posts: 3253
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 11-3-2004 at 21:08


Back in high school we took KClO3 and added it to water till a considerable amount dissolved. Then we heated with a bunsen burner (it was in a large test tube) till it all dissolved and waited, after a bit a rainbow of crystals came out of solution, it was incredibly stunning to watch.

Also with KClO3 we took a bit and melted it in a large test tube over a bunsen burner, then dropped in a gummy bear, it bounced all around and shot up purple flames, it was called "The Gummy Bear Goes to Hell" ahhh I think I'll do that one again next week....




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
tom haggen
Hazard to Others
***




Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline

Mood: a better mood

[*] posted on 11-3-2004 at 21:22


Some of my first experiences with crystallization was with KCLO3. I found that its much easier to get the crystals to form than it is with nirtate salts. nitrates stay molten very easily. I haven't really worked with molten KCLO3, that gummy bear trick sounds cool. I think i might try it.

[Edited on 12-3-2004 by tom haggen]




N/A
View user's profile View All Posts By User This user has MSN Messenger
chloric1
International Hazard
*****




Posts: 1146
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 23-3-2004 at 10:29
Perchloric acid


It took me years to get perchloric acid. Until I was able to buy it, I made it. If you are in fact in the US you can buy ammonium perchlorate from pyro suppliers. It runs $10 per pound but more than worthit! If you make aqua regia with nitric and hydrochloric acids, you dissolve the AP crystals and let them sit for about 24 hours. Once reaction commences, leave it alone! It is safest to keep this mixture cool until the ruby-brown color disappears. Once it achieves a clear yellow this signifies that the ammonium ion in decomposed completely. Now cautiously heat the mixture and distill off the HCL, chlorine, and Nitric acid. Excellent ventalation is imperitive! Do this until no more smokey fumes come off. This will be your crude HClO4!! I hope this helps!:D

[Edited on 3/23/2004 by chloric1]




Fellow molecular manipulator
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 23-3-2004 at 12:51


Great idea!
Sadly though, it still contains other acids :(
Plus, if you start off with KClO4 instead, it's even harder to get salt-free HClO4..
But that's off topic I know. Maybe I should have a look at the perchloric acid thread again!




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 23-3-2004 at 14:04


Could you electrolyze a solution of ammonium perchlorate? Or use a salt bridge for a metal perchlorate salt?
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


[*] posted on 23-3-2004 at 15:20


I wouldn't want to electorlyze anything that had both ammonia and chlorine in it for fear of creating nitrogen trichloride. In theory, electrolyzing a solution of potassium perchlorate should work. Subject to the usual difficulties when trying to produce an acid by electrolysis.
View user's profile View All Posts By User
Theoretic
National Hazard
****




Posts: 776
Registered: 17-6-2003
Location: London, the Land of Sun, Summer and Snow
Member Is Offline

Mood: eating the souls of dust mites

thumbup.gif posted on 24-3-2004 at 02:20


On the topic of obtaining HClO4 via AP and aqua regia... If the ammonium ion is decomposed by chlorine from aqua regia (due to the equilibrium 3HCl + HNO3 <=> NOCl + Cl2 + 2H2O), then either nitrogen evolves and hydrogen chloride is made (plus NOCl from the shifted equilibrium, which is chemically reactive and does mess up your final product but is volatile and can be distilled off), or, alternatively, nitrogen trichloride is made (with excess chorine), which can (and often does) explode! It can decompose to nitrogen and chlorine safely, but this still wastes aqua regia.
An alternative is to add ferric chloride to your AP solution to form NH4Cl and ferric perchlorate, dry it out and heat cautiously untill all the ammonium chloride distills away, then put it into hot water and dilute untill it hydrolyses and Fe(OH)3 precipitates, filter and you're there (or so I hope)!
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1146
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 24-3-2004 at 19:55


Yes Theoretic i like your metal salt hydrolysis but it really would be hard removing the iron. Yes you are right about a potential explosion hazard! That is why perchlorate manufacturers abandoned the batch process but if you keep the quanties under 500ml you ahve reduced risk. And remeber what I said about the red color in the last post! Dont heat it ,throw it against brick walls,add other chemicals or expose to direct sunlight! Just let it chill out for about 24 to 48 hours and the oxidizers in solution will take care of your ammonium ion for you. Just rember clear yellow is all is safe and clear and red is for danger!:o:o



Fellow molecular manipulator
View user's profile View All Posts By User

  Go To Top