cyclic diester
I have dimethyl ester ofadipic acid and ethylene glycol to make a cyclic diester (MSA is catalyst). any suggestions how one can avoid making a
polymer?
|
|
sonogashira
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 555
Registered: 10-9-2006
Member Is Offline
Mood: No Mood
|
|
High dilution with ethylene glycol will make cyclization more probable, but i do not know if the yield will be very high even still. Are 10-membered
rings are very favorable? I would not imagine but i am not sure. But it is a known product i assume?
[Edited on 4-8-2009 by sonogashira]
|
|
sparkgap
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline
Mood: chaotropic
|
|
Remember that forming rings larger than five or six atoms is not as kinetically or thermodynamically facile. I suggest looking into past work, e.g. http://www.google.com/patents?&vid=USPAT2092031&id=7... ![:)](./images/smilies/smile.gif)
HTH
sparky (~_~)
"What's UTFSE? I keep hearing about it, but I can't be arsed to search for the answer..."
|
|
JohnWW
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
Because of the mutual angle for tetrahedral sp3 bonding of 109º28', 5-membered (108º) and after that 6-membered (120º) rings are usually most
favored energetically, if all four groups attached at the central sp3 atom are of similar size and polarity. Even then, 6-membered rings, and even
more so 7-membered and larger rings, with all single bonds,, flex considerably out-of-plane in order for the constituent atoms to approach a bonding
angle close to 109º28'.
[Edited on 5-8-09 by JohnWW]
|
|
ProChem
Harmless
Posts: 41
Registered: 9-6-2008
Location: Union Beach, NJ. USA
Member Is Offline
Mood: Cynical
|
|
Shortly after I posted the question I found many patents I reacted sebacic acid and ethylene glycol (EG) with ptsa to make a polyester. The second
step I heated the polyester with titanium isopropoxide under vacuum. Success! the next project I used 1,4-butane diol instead of EG. This time it
didn't work however I collected THF as a product.
|
|
ammonium isocyanate
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 124
Registered: 13-7-2009
Location: USA - Midwest
Member Is Offline
Mood: sick
|
|
Could we see a write-up of your reaction?
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by ProChem ![](images/xpblue/lastpost.gif) | Shortly after I posted the question I found many patents I reacted sebacic acid and ethylene glycol (EG) with ptsa to make a polyester. The second
step I heated the polyester with titanium isopropoxide under vacuum. Success! the next project I used 1,4-butane diol instead of EG. This time it
didn't work however I collected THF as a product. |