Chlorate the other way
Supposed I have enough conc. HCl, as well MnO2 and NaOH OR Ba(OH)2 :
Could I just make a hot solution of hydroxide, bubble in the chlorine and ready ? Could be quicker than waiting for a tedious electrolysis to get
finished ?
[Edited on 17-4-2009 by chief]
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
You can make chlorate in this way if the solutions are hot, but the trouble is that only 1/6 of all chlorine ends up in chlorate, the other 5/6 end up
in chloride. Isolating the chlorate from such dilute solutions is not easy, especially if you have the highly soluble chlorates of sodium or barium.
This works better with KOH making KClO3.
With electrolysis you make chlorate (through the intermediate of hypochlorite) but there you continue with making chlorine as long as chloride is
present. So, in electrolysis you finally use up all chloride, converting it to chlorate.
|
|
hissingnoise
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
If we knew what exactly the fire suppressants in chlorate weedkiller are, it might be possible to separate them by fractionation. . .
Thermal oxidation to NaClO4 produces 1/3 NaCl which is manageable.
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
We do know that, the MSDS tells you. In the EU, where the products look to be going away in the next year or so, the main additive is NaCl.
In the US it is generally sodium metaborate, which has a solubility somewhat similar to sodium chlorate. Adding the correct amount of boric acid
converts the metaborate to borax, which has a much lower solubility in cool and cold water and gives decent separation.
Calcium chlorate is also used, at the time it was accessible where I was living the additives varied greatly, it was a bag by bag decision on how to
clean it up to get Na or K ClO3.
|
|
Nick F
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 7-9-2002
Member Is Offline
Mood: No Mood
|
|
In all brands of chlorate weedkiller that I've come across the sodium chlorate crystals are bigger than the fire suppressant crystals, so mechanical
sieving gives pure sodium chlorate. Use the coarsest sieve possible, to ensure that it only retains chlorate. The weedkiller container will tell you
what % chlorate it is. So then you weigh what you sieved out, work out how much chlorate is still left in the fire suppressant, and use KCl or KNO3 to
precipitate the rest of the chlorate as KClO3 which has low solubility in cold water.