xxxxx
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 21-5-2004
Member Is Offline
Mood: No Mood
|
|
flexible/elastic cyanoacrylate glue?
cyanoacrylate glue is wonderful stuff, unless you wish to join flexible or elastic materials which will be bending or stretching. then the rigid,
crystalline glue will gradually crumble to bits breaking the bond. i would like to ask if they couldn't put an ether or an ester linkage on the
monomer to make the polymer elastic and flexible while still retaining the adhesion confered by the cyano linkage.
|
|
sparkgap
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline
Mood: chaotropic
|
|
The cyanoacrylates sometimes used in surgery form quite flexible polymers.
It doesn't have to be an ether or ester linkage. It only has to be such that the packing of the resulting polymer is not extensive and dense,
implying that the starting material should be a "some random medium-sized group" cyanoacrylate. ![:)](./images/smilies/smile.gif)
sparky (~_~)
P.S. Interesting, this is.
"What's UTFSE? I keep hearing about it, but I can't be arsed to search for the answer..."
|
|
xxxxx
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 21-5-2004
Member Is Offline
Mood: No Mood
|
|
i know this is a post on an old thread but locktite has begun public sale of a flexible cyanoacrylic adhesive. you can get the 20 gram bottle for
about us$20 if you shop around. i have not tried this stuff yet. maybe someone could buy some and post a review.
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
I have a pressure activated superstrong adhesive I use for splicing flylines. I believe it to be a cynoacrylate and will look it up to determine
whether that's the case.
Mine is indeed another Locktite cyanoacrylate:
http://www.wentite.com/jscs/sgj/Product_414.pdf
[Edited on 1-3-2009 by chemrox]
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|