Author: Subject: cheap copper electrodes
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 23-10-2008 at 11:51
cheap copper electrodes


cheap copper electrodes are available at American Science & Surplus. They sell a 53/4" X 3/4" X 0.41" strip for $2.

sciplus.com




"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1240
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 23-10-2008 at 16:56


Not exactly cheap but I'll make note of that.



Fellow molecular manipulator
View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 23-10-2008 at 17:23


Whats so great about copper electrodes vs copper pipes?

Oh yeah.. and Happy mole day :P

[Edited on 23-10-2008 by kclo4]
View user's profile Visit user's homepage View All Posts By User
crazyboy
Hazard to Others
***




Posts: 436
Registered: 31-1-2008
Member Is Offline

Mood: Marginally insane

[*] posted on 23-10-2008 at 20:23


Quote:
Originally posted by kclo4
Whats so great about copper electrodes vs copper pipes?

Oh yeah.. and Happy mole day :P

[Edited on 23-10-2008 by kclo4]


Yeah I just use a copper pipe I cut open and hammered flat.

My chem teacher gave us chips and guacaMOLE (no joke.)




View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 23-10-2008 at 21:14


Interesting! I never thought of Hammering them out, I have just always used them as is.

What exactly are the benefits for them being into a flat sheet? I assume surface area or something like that, but I don't know if that really matters very much.

erm... I guess if your cell structurally "favors" a certain shape it would matter.
View user's profile Visit user's homepage View All Posts By User
crazyboy
Hazard to Others
***




Posts: 436
Registered: 31-1-2008
Member Is Offline

Mood: Marginally insane

[*] posted on 24-10-2008 at 14:45


I hammer it out because if I use it for several runs I can easily clean it with a bench grinder plus it makes it easier to drill a small hole in it where I can put a wire.



View user's profile View All Posts By User
smuv
National Hazard
****




Posts: 842
Registered: 2-5-2007
Member Is Offline

Mood: Jingoistic

[*] posted on 24-10-2008 at 15:47


I think considering the thickness the price is reasonable, not wonderful. At any rate, nice of you to share.

@ crazyboy, if you have a torch, you would probably get more consistent results if you just soldered the wire to the electrode.




"Titanium tetrachloride…You sly temptress." --Walter Bishop
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 27-10-2008 at 19:40


Using 559 lb/cu-ft as the density for copper, it comes out to $38.76/lb. That's downright expensive, unless you need just one or two and have no better source. I get surplus stock copper in my area for $3.50/lb.
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 27-10-2008 at 19:50


Copper electrical wire is supposedly very pure for efficient conduction reasons. There is enough 1-2mm diameter wire lying around in construction site junkheaps that I have never bought.

A flat electrode is preferable if one is doing analytical work, as it will have a uniform current density over the surface when the other electrode is beside it. For uniform current density on a cylinder one needs another cylindrical electrode around it, and of course spacing must be precise.




View user's profile View All Posts By User
grndpndr
National Hazard
****




Posts: 508
Registered: 9-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 30-10-2008 at 10:14


Not to defend American science and Surplus but some of thier(limited) glassware is reasonable/good range of useful surplus electronics and customer service fine. Instead of returning a broken 500ml broken seperatory funnel, it was simply replaced with a phone call.Chinese,but 'adequate'.:)

Copper pipe would seems the material of choice partcularly since scrounging yields far more useful things than one would first imagine.

[Edited on 30-10-2008 by grndpndr]

[Edited on 30-10-2008 by grndpndr]

[Edited on 30-10-2008 by grndpndr]
View user's profile View All Posts By User