What force is needed to deform gold ?
Hello,
I am doing some personal research on what force is needed to deform a certain metal. In fact, I want to know how much force is needed to press a small
gold bar.
I looked on the internet about a certain formula that I could use to calculate it but I had no success. The closest formula I found is the Young's
modulus formula but it does not seem to be appropriate for this application, since I end up with 1 000 000 pounds needed lol.
Please fellow chemists or physicists, help me !
Thanks in advance.
Knowledge is the Key.
|
|
chief
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 630
Registered: 19-7-2007
Member Is Offline
Mood: No Mood
|
|
There is such a thing as the "hardness" or "microhardness" of a material, the unit is that of pressure, usually GPa.
If something has a hardness of eg. 5 GPa, then it will not deform below about that pessure, which would mean: 5 GPa == 5 GigaNewton/m^2 == 50000
kg/cm^2 == 50 kBar.
That sort of hardness is usually measured by means of a special microscope, that allows applying a force (diamond-tip) onto the sample, and then
measure the crater ...
But it's a raw approximation, since materials have all sorts of elacticity, get harder under pressure (nonlinearity), ...
|
|
noxx
Harmless
Posts: 25
Registered: 27-12-2007
Location: Québec, Canada
Member Is Offline
Mood: Raffinate
|
|
Ok I see. But is the harness the minimum force needed to deform (flatten) a metal ?
Thank for the answer.
Knowledge is the Key.
|
|
watson.fawkes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by noxx
I am doing some personal research on what force is needed to deform a certain metal. In fact, I want to know how much force is needed to press a small
gold bar.
I looked on the internet about a certain formula that I could use to calculate it but I had no success. The closest formula I found is the Young's
modulus formula but it does not seem to be appropriate for this application, since I end up with 1 000 000 pounds needed lol. | To press it all at once? Yeah, it's a lot of force. How is gold actually worked? Pressed on not all at once. See "peening".
|
|