I was busily making some sodium metal via electrolysis of NaOH when I decided to attempt using a steel (non-stainless) anode. The result was the
formation of a green mineral-like compound that appears to be deliquescent. Discerning the identity of the compound is likely quite simple, however
since it is a pretty compound, I thought I'd post the pictures of it here.
![](http://img510.imageshack.us/img510/5084/img4207ls0.th.jpg)
![](http://img390.imageshack.us/img390/6779/img4215ox4.th.jpg)
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Ferrite?
|
|
ShadowWarrior4444
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 226
Registered: 25-4-2008
Member Is Offline
Mood: Sunlight on a pure white wall.
|
|
Quote: | Originally posted by 12AX7
Ferrite? |
As in transformer-core ferrite? Those are ostensibly iron-oxide ceramaics, usually not green or soluble.
I suspect some sort of sodium-iron compound, perhaps somewhat analogous to Prussian blue. A sodium-iron mineral of sorts? It dissolves into a green
solution, though. The green color indicates Fe2+, the rest is perhaps some mixture of Na, O, and OH. Due to its hygroscopic nature, I suspect OH
groups to be present.
I should also note that the black on the bottom of the green is most likely an accumulation of carbon, or other various metals that were in the iron
alloy. (MnO2?)
An update:
After a short while in a petri dish--
![](http://img510.imageshack.us/img510/875/img4219sg9.th.jpg)
![](http://img374.imageshack.us/img374/1097/img4220uh2.th.jpg)
And a tryst on some cast iron:
![](http://img77.imageshack.us/img77/8190/img4221kh9.th.jpg)
Interestingly, any of the compound left on the cast-iron seems to turn from green to yellow/off-white, perhaps due to some catalytic oxidation via
Fe2O3.
It also seems that the substance (revised term) is only partially deliquescent; the green (iron component) seems to dissolve into solution, leaving
behind a mineral-like white substance. Unless this is simply an illusion created by the atmospheric oxidation of the outer layers.
All pieces are also completely non-magnetic, as tested with N48 magnets-of-doom.
[Edited on 7-11-2008 by ShadowWarrior4444]
|
|
JohnWW
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
That lime-green color is characteristic of the hydrated Fe(II) cation, Fe(H2O)6++, which however is free from hydrolysis only in acid solution. It is
unclear what the associated anion could be, if that is what it is. Because of the strongly alkaline environment from which it came, molten NaOH, it is
more likely to be instead a sodium ferrite(II), possibly as [Fe(OH)4]-- or [Fe(OH)6]4-. Sucjh a species would be very liable to oxidation to Fe(III)
by atmospheric oxygen.
|
|
ShadowWarrior4444
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 226
Registered: 25-4-2008
Member Is Offline
Mood: Sunlight on a pure white wall.
|
|
Quote: | Originally posted by JohnWW
That lime-green color is characteristic of the hydrated Fe(II) cation, Fe(H2O)6++, which however is free from hydrolysis only in acid solution. It is
unclear what the associated anion could be, if that is what it is. Because of the strongly alkaline environment from which it came, molten NaOH, it is
more likely to be instead a sodium ferrite(II), possibly as [Fe(OH)4]-- or [Fe(OH)6]4-. Sucjh a species would be very liable to oxidation to Fe(III)
by atmospheric oxygen. |
Incidentally, what is the most commonly accepted deffinition of a ferrite--"An unstable compound of a strong base and ferric oxide which exists in
alkaline solution, such as NaFeO2," an iron-containing material with a body centered cubic structure, or "a class of chemical compounds with the
formula AB2O4, where A and B represent various metal cations, usually including iron."
I should mention that during the electrolysis, the steel anode did bubble vigorously. I also found that at times a closed circuit was formed,
requiring the anode to be raised slightly in order to continue the electrolysis. In addition, when molten this substance was tan/brown, it was only
upon cooling that it turned green.
|
|