anhydrous calcium chloride
I have some calcium chloride hexahydrate but need to convert it to a good anhydrous desiccant, as far as possible. What is the optimum temperature to
heat it to and for how long.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Don't bother with the temperature. Just throw it on the stove til it stops evolving steam and becomes a dry powder
I heard it loses its water at ~175C.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
mechem
Harmless
Posts: 32
Registered: 27-12-2007
Member Is Offline
Mood: No Mood
|
|
Would it not stay at the dihydrate at 175C
|
|
Phosphor-ing
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline
Mood: Inquisitive
|
|
http://www.physicsforums.com/archive/index.php/t-174878.html
tells you what happens at 175C
[Edited on 17-4-2008 by Phosphor-ing]
"The nine most terrifying words in the English language are: 'I'm from the government and I'm here to help.'" -Ronald Reagan
|
|
Klute
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1378
Registered: 18-10-2006
Location: France
Member Is Offline
Mood: No Mood
|
|
I'm sure it would be much easier to just go and buy the anhydrous pellets in any hardware store, no? These work wonders as dessicant for dessicators,
gas, and certains solvants/solution (check compatibility beforehand).
They are very cheap, it will surely be more expensive to heat up a oven at >200°C for several hours to get a few 100's g of product.
|
|