Luciangamer
Harmless
Posts: 6
Registered: 9-10-2007
Member Is Offline
Mood: No Mood
|
|
Capillary tubes
Where can the capillary tubes like the ones used in lab be purchased? All I found on ebay were things that looked some type of biomedical equipment
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
try a Web search, find lots of places like
http://www.sciencelab.com/page/S/PVAR/10615/10-2430-34
http://sciencekit.com/product.asp?pn=IG0026111&bhcd2=119...
|
|
Luciangamer
Harmless
Posts: 6
Registered: 9-10-2007
Member Is Offline
Mood: No Mood
|
|
Thanks, that is exactly what I was looking for
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
It's pretty easy to make them yourself from glass rods using a MAPP torch for example.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Vulture, how do you dril the hole through a rod?
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
What? We just order hollow rods with an inner diameter of approx 5mm. They're pretty cheap and make good capillary tubes (with some skill) for vacuum
distillations.
[Edited on 16-12-2007 by vulture]
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
A rod is solid; a tube has a hole through it.
|
|
Ozone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
I have always used cheap, disposable Pasteur-type pipettes. They are only a few dollars for a large box. Simply rotate over a nice blue flame until an
organge glow is imparted to the flame and the glass begins to sag slightly. Then, firmly, but smoothly pull the ends apart. You should get a very
fine, hollow tube suitable for TLC spotting which can be broken into as many smaller parts as needed. Expect at least 30 spotters per-pipette.
Don't worry when you frag ther first few. They are cheap.
Cheers,
O3
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|
dangator
Harmless
Posts: 8
Registered: 22-1-2008
Member Is Offline
Mood: No Mood
|
|
As a follow-up to ozone--you want the -flint glass- pipettes for easy pulling with a typical bunsen burner.
|
|