How thick can an anodized layer be?
In the aluminum anodizing process, does the oxide layer grows indefinitely as long as current flows? Or how thick can it get?
My intention is to anodize a tube to electrically insulate it. This way I can wind Ni-Cr wires directly around it to make a mini hot air gun.
Thanks.
|
|
jpsmith123
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 764
Registered: 24-6-2005
Member Is Offline
Mood: No Mood
|
|
Hello Tacho,
I admire your resourcefulness, but is it worth it to even fool around like that when you can get a heat gun for $10.00? (I would think in Brazil there must be something similar?)
Anyway, here's an article from the Electrochemistry Encyclopedia that might be helpful.
One concern I would have would be the difference in thermal expansion between the metal and the oxide, especially if the oxide were thick and subject
to repeated thermal cycling.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Hardcoat may suffice. I know electronics professionals (good ones ) who have
been known to mount transistors on hardcoat heatsinks. It's also very thermally conductive, being aluminum oxide.
Aluminum goes up to 500V or so- think aluminum electrolytic capacitors. As the anodization grows, the voltage must be increased.
Tim
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
Thank you.
The link ( Electrochemistry Encyclopedia ) is the best information on anodizing I have seen so far.
My Idea is really a small scale thing and, as Tim pointed out, oxide insulation layers can be useful in many other projects. Besides, I really never
saw one of those for sale for U$10 (or equivalent). Bless China.
|
|
Nixie
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
Quote: | Originally posted by 12AX7
It's also very thermally conductive, being aluminum oxide.
|
Bah, you can get beryllia insulators from eBay.
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
You can get a fair few carcinogenic things on eBay if you look hard enough.
I don't know how thick a layer you can get but there's another neat trick you can do. You can anodise a layer of oxide onto the Al then dissolve away
the Al from the other side with I2 soln. That way you might get an Al2O3 tube without the metal.
|
|
Nixie
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
Quote: | Originally posted by unionised
You can get a fair few carcinogenic things on eBay if you look hard enough. |
How is it carcinogenic? Only the dust is. Cut/drill under water and it's perfectly safe (the diamond bits you need to work this hard ceramic are