Visible silver particles?
I`m not sure if this belongs in Here or Energetic materials, but anyway...
I`m conducting an Old experiment, that consists of making my own photographic paper (coffee filter paper soaked in silver nitrate and then NaCl soln
and allowed to dry).
now this works great in sunshine (reacts in Minutes).
but what I`m doing is using and Isotope to expose this paper that is in a dark envelope, with a wire mesh on that and then the Isotope.
I`m hoping that if it works I`ll get a clear(ish) mesh pattern appear on the paper.
this sample I have gives off 1200 DPS, and I calculate that over a week I should have nearly 73 million "hits" to the paper.
would that be Visible at all?
it Sounds like a lot of hits, but in atom sized silver particles it isn`t really that much I don`t think.
the area it will be over is roughly 3cm x 3cm.
it`s also in a Light and air tight box, I`m wondering if Radon may make the paper blurry also, as it`s resting at the bottom of this box.
I`m sure Someone here has done all this before and knows the score, and can hopefully provide a little help/guidance.
if it works, I`ll put some pictures up also!
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Assuming that DPS stands for decompositions per second, and that one particle appears per decomposition I find roughly 104 million particles per week.
How much of these hit the paper is not easy to tell, but let's assume 25%, then you'll have 26 million hits per week.
This is an amazingly small amount. If you think about the number of atoms in a mole, which is 6.02*10^23, then you see that you only have in the order
of 10^(-16) to 10^(-15) mole, which is in the order of magnitude of 0.01 picogram to 0.1 picogram. I would be surprised if you see any difference
between the exposed area and the rest of the paper. A picogram is VERY VERY small.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
well I don`t know the Total DPS as in all 720 degrees of the isotope, the 1200 count is from a single side of it.
it will penetrate and pass through lead though 3mm thick.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
If it passes through lead 3 mm thick, then only a tiny fraction will be captured by your AgCl-paper and then the situation is even worse.
I am afraid that it hardly will be visible. With a developer (such as hydroquinone + Na2SO3 + metol) things can change a lot. A single silver atom,
excited by light (or other radiation) acts as a nucleation spot, where the developer attacks the silver chloride much more easily than on other
places. This is the basis of photography. The silver particles themselves are invisible, but they allow much faster reduction of nearby AgCl, compared
to other AgCl. These invisible silver particles form a so-called "latent image". Search google for "latent image", one fairly good link is this one:
http://en.wikipedia.org/wiki/Latent_image
Hopefully this helps and gives some more understanding. This is very interesting matter. Even better results are obtained with mixed AgCl/AgBr
deposits.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
that`s Great help thanks ![:)](./images/smilies/smile.gif)
I have the Hydroquinone and sodium sulphate is easy enough to knock up in a few mins.
I considered the Bromide also, but not having a Proper "dark room" in which to dry these papers or handle them, I figured the Chloride would be best
as it`s pretty forgiving to low light and short exposures, I think the bromide is more sensitive.
I think maybe the best thing I can do is Check it at the end of the week and see if there Is any change, and if not leave it for Longer.
it`s not really costing me anything to do this, only filter paper and some space.
and although I`m excited about hopefully getting a result, I`m more than Patient when need be.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
"I have the Hydroquinone and sodium sulphate is easy enough to knock up in a few mins."
No sulfate, but sulfite must be used. It also is important to use normal sulfite and not a bisulfite. The solution should be mildly alkaline,
otherwise it will not work.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
aha yes, I didn`t see the 3 and assumed 4, Thanks, My Bad ![:)](./images/smilies/smile.gif)
NaOH soln and SO2 bubbles though it? should work I believe?
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Do you have bisulfite? If you have that, use some excess Na2CO3 or K2CO3 and the bisulfite. You also could bubble SO2 through a solution of Na2CO3,
but that is more hassle. For SO2-production you could use copper wire in H2SO4, although a large excess of H2SO4 is needed. Using Na2CO3 instead of
NaOH assures that the solution is only mildly alkaline, otherwise it is strongly alkaline.
Hydroquinone in a strongly alkaline solution really sucks. Just for fun, try it. The hydroquinone then is oxidized by oxygen from air within a few
minutes, it really sucks oxygen from the air and before your AgCl is developed, the hydroquinone already is spoiled if the pH is too high.
For developing a print of 10x15 cm, you only need 100 ml or so of liquid, with only 100 mg or so of hydroquinone added and a gram or so of sulfite.
Solutions only need to be dilute.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
I make the SO2 in a Large flask, it has a spoon that I put Sulpher onto and light, this then goes into the flask and the air pipe feeds the flame and
the pipe Out has the SO2.
it`s nothing fancy, just something I made myself with some glass tubing a fish tank pump and some scrap SS metal bits, but it serves me well ![:)](./images/smilies/smile.gif)
I don`t have any bisulphite at all, so I shall have to make some, but`s good too and I don`t mind doing that ![:)](./images/smilies/smile.gif)
that High PH and HQ sounds like a nice way to make Nitrogen! (if you ignore a little Argon).
I have all these carbonates (and more) that you mention, and I have at least 1 week to make some of these things needed, I think it will add Extra
appeal and interest to the project when you consider that even the Silver Nitrate was made by me and the photo paper etc...
Really RETRO-TECH
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
garage chemist
chemical wizard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline
Mood: No Mood
|
|
The SO2 gas that you make should better be free of oxygen, since oxygen rapidly oxidises solutions of sulfites.
This is a big problem in industrial production of sulfites, here the residual oxygen in the sulfur burner gas quantitatively reacts with the sulfite,
leading to a considerable loss. Pure SO2 gas would be uneconomic to use due to its much higher price, and sulfur stops burning if the oxygen content
of the gas drops below a certain value.
They separate sulfite and sulfate by fractional crystallization (Na2SO4 as the decahydrate, by cooling) and sell the sodium sulfate byproduct as well,
after refining to normal purity standards.
I recommend you to buy some sodium disulfite (also called metabisulfite or pyrosulfite), it is a highly useful chemical, especially in inorganic
chemistry.
The only good way to make sulfites at home would be to liquify SO2 from the burner gas using dry ice, or using a different chemical method to make
pure SO2 (like reduction of H2SO4 with copper or other metals- gives useful byproducts depending on what you use) for reaction with your base.
[Edited on 15-11-2007 by garage chemist]
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
I have Kipps apparatus here, it probably wouldn`t take too much effort to "fire it up" and get it working again.
although the acid, does it have to be Conc sulphuric? I only have about 500ml of that left!
I have also Campden tablets, they give off SO2 when added to water, theyr`e used as sterilisers in Beer or Wine making.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
garage chemist
chemical wizard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline
Mood: No Mood
|
|
I would hardly call a Kipp suitable. The reduction of H2SO4 requires strong heating. Just use a normal flask or erlenmeyer.
500ml is plenty, you'll probably need only 50ml to make the SO2 you need.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Campden tablets are mainly bisulphite anyway, you might be able to use them directly.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Yes, the campden tablets are almost pure K2S2O5. I have the powder form of this and it states as the ONLY ingredient potassium metabisulfite. But if
you are not sure, then use these tablets to make SO2. Mix 1 volume of H2SO4 with 1 volume of water (careful, hot!!) and then add crushed tablet.
Slight heating is required (60 C or so). SO2 is bubbling off.
But, first I would try directly, dissolving some of the crushed tablet in a solution of Na2CO3, keeping the solution alkaline.
But as garage chemist did, I also really recommend you to either buy sodium sulfite by the kilo (available from silverprint) or some metabisulfite
(available at shops, who have wine making stuff, the usually carry the potassium salt). Sulfite (or one of its variations) is one of those chems,
which I really consider a baseline chem and which should be present in a serious home lab.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
ok, I went out today and got a pretty good deal on some proper 35mm film, 3 rolls for 97p!
ok it`s a little out of Date sure, 9/07.
but it`ll probably do a better job than my coffee filter paper and Silver Chloride I expect.
it`s a 36 shot film and ISO 200/24(degree symbol) 135DX/36 whatever that means??? (sounds like a Processor spec! LOL).
so my plan is to get somewhere totally dark, unravel this film and cut it into single sheets and then store them in a light tight tin, and take them
out as I need them and put then in black paper and try from there.
I`m assuming I will need the same stuff to develop them???
the Good part is that I have a projector that will show these negatives so I may be able to see more detail than I would with my filter paper method
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
135 is the size/type of film cassette DX means there's a coding on the edge of the film to tell suitably equipped camaras what film speed it is and 36
is the number of exposures.
http://en.wikipedia.org/wiki/DX_encoding
This could be a dumb question; is it monochrome or colour film?
The developers for colour film are more complex.
Also I just wondered, if you put a few layers of the film on top of eachother before exposing them would they have a better chance of catching the
gammas and recording an image?
(It might be a bit tricky to keep them lined up)
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
not dumb at all, it`s a Color film.
Samsung Prime Color Film, to be exact.
your Layering idea is Good actually, I expect that with alu plates or maybe even thin lead, it might be possible to create a 3D type of effect, a bit
like a CAT or MRI scan?
[Edited on 17-11-2007 by YT2095]
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I'm not sure how you would develop the colour film. Taking it to the local photographic shop and saying it's a radiograph might get some funny looks.
I would try to find some black and white film on ebay.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
well for the Original experiment with the silver chloride paper I made, it`s failed entirely, there`s not even a Trace of exposure, and what`s worse
is that when I took it out the black envelope it was Wet too.
the Sodium nitrate part has obviously taken in moisture from the air and ruined it (assuming there was anything to ruin).
nevermind, I`ll know better for Next time
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Color film development is VERY different from B&W development. You need a rather extensive set of rare chemicals, which are hard to obtain. Color
films have different dyes in the emulsion layer, which are developed by light of different wave lengths. This makes color development a rather picky
process, which only works under highly controlled conditions (e.g. temperature control with an accuracy of 0.1 C or so) and for this reason only the
most experienced and advanced hobby photographers do color development at home. It is possible, but not easily done.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
so basically I`m doomed then unless I get hold of some B/W photo paper.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
You can develop colour film as B/W, it is still a silver halide base material. The colour part uses the byproducts of developing the silver to couple
with chemicals in the developers to form dyes. If you did around on the Net some I suspect you'll be able to find some information on that.
For DIY, these might be useful
http://www.artic.edu/~fendsley/altProc_SaltPaper.html
http://www.alternativephotography.com/process_albumen_paper....
http://unblinkingeye.com/Articles/Emulsion/emulsion.html
http://www.apug.org/forums/forum205/32860-notes-account-maki...
http://www.iop.org/EJ/abstract/0950-7671/23/5/304
http://www.archive.org/details/chemistryofphoto00harruoft
Real world books that could be of interest
http://www.christopherjames-studio.com/build/thebook.html
Photographic Emulsion Technique
http://www3.interscience.wiley.com/cgi-bin/abstract/11276696...
Note that the old plates and less modern print material are rather insensitive. Your 1200 DPS source could take weeks to months to expose. When I
was young I had a 'science kit' that included a radioactive source, probably a few hundred DPS; the experiment making what you want to do took a
couple of weeks of exposure using B/W sheet film.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
That`s Fantastic news! Thank You! ![:D](./images/smilies/biggrin.gif)
I got a little concerned for a while because I was considering buying More of these films, and although they`re not expensive it would have been quite
wasteful.
I`ve got all morning free tomorrow, so I`ll go through those links and take a few notes as well as finish my Dark room and red light array (I`ll be
using LEDs).
would I be correct in saying that I will need to wear gloves while handling the raw unexposed film, and also will I be able to see the marker between
each shot? this a 36 picture film, will the line between each be clearly visible in red light?
I want to cut the film into single plates so I can use them one at a time, the reason is that a Radiation source may affect the entire roll just for
taking one picture, so a single piece of film per exposure would be best.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Quote: | would I be correct in saying that I will need to wear gloves while handling the raw unexposed film, and also will I be able to see the marker between
each shot? this a 36 picture film, will the line between each be clearly visible in red light? |
No, the emulsion coating is continuous, the frames that show up after developing are caused by unexposed film.
I'd find some instructions on developing colour film as B/W before buying any more, though.
[Edited on 23-11-2007 by not_important]
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
this just gets better then! so I may even get 37-38 slides from it ![:)](./images/smilies/smile.gif)
and even try a 360 wrap around to get a complete idea of emissions from this "hot rock"
and thinking about it color would be a little useless anyway for this type of picture.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
Pages:
1
2 |