H2PtCl6 decomposition
A paper says H2PtCl6 will decompose if heated, but no details.
I wonder at what temperature H2PtCl6 will decompose? and what is the decomposed product? I guess Pt, HCl, Cl2?
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Brauer (see our library) gives the preparation of PtCl4 from H2PtCl6, stating "the temperature must not be allowed to rise above 360°C". Since it
must be dried in a stream of hot Cl2 gas, it's reasonable to assume it will decompose beyond 300°C or so into a mixture of platinum oxides,
chlorides, and perhaps some metal as well.
Tim
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
It usually decomposes into a lower chloride. It will not decompose into its oxide Tim, not with Pt. It will actually go to metal first. I have a post
coming soon that should address all of these Pd and Pt questions people seem to be having here, with gratuitous color photos!