Frozen Glass joint?
well I made out like a Bandit today in glassware and half of it I have no idea what it`s even for!
but the Kipps apparatus I have has a badly frozen ground glass joint as it`s been sitting on a shelf for several decades without being properly
cleaned.
HOW do I get the thing apart?
brute force doesn`t seem to work, and I don`t want to break it.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
evil_lurker
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline
Mood: On the wagon again.
|
|
Try gentle heat from a heat gun first.
If that does not work, then send it off to a glassblower... its not worth ruining such an expensive and hard to find piece.
Not all chemicals are bad. Without chemicals such as hydrogen and oxygen, for example, there would be no way to make water, a vital ingredient in
beer.
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Save your money use WD40 let it penetrate well and problem resolved......solo
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7990
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Take a little WOODEN hammer (a toy hammer may also work). Wrap the stuck joint in thin tissue paper and carefully tap the joint, while someone else
carefully tries to pull things apart. This works in many cases. But DO NOT use a metal hammer. That will break the delicate glass. A metal hammer is
too heave.
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Have you tried running boiling hot water over the outer joint- just long enough to warm it but not heat the inner one?
This usually works for me- if it doesn't WD40 as the man said.
|
|
jam640
Harmless
Posts: 29
Registered: 3-10-2007
Location: Rainbow Island
Member Is Offline
Mood: Fat
|
|
If gentle heating doesn't work you may try applying a small amount of methanol which usually slowly soaks in between the glass and let's it loose.
|
|
evil_lurker
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 767
Registered: 12-3-2005
Location: United States of Elbonia
Member Is Offline
Mood: On the wagon again.
|
|
Actually I bet some stuff called Penetrating Blaster would work great.
Its similare to Liquid Wrench for getting nuts and bolts off, cept it works much better.
You can get it in Wally World or many fine auto parts shops.
Not all chemicals are bad. Without chemicals such as hydrogen and oxygen, for example, there would be no way to make water, a vital ingredient in
beer.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
I hear tell PBlaster is mostly ATF and lacquer thinner. WD40, likewise, is essentially mineral spirits; to be exact, it's a lot of stoddard solvent,
plus a little oil which remains when the solvent dries.
Edit: among the organic laboratory, anything etherial (light alkanes, ethers, ketones, etc.) with something oily, waxy or fatty dissolved in it would
probably suffice.
Tim
[Edited on 10-5-2007 by 12AX7]
|
|
Antwain
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 252
Registered: 21-7-2007
Location: Australia
Member Is Offline
Mood: Supersaturated
|
|
When I seized a joint (and cracked the attachment off a thermometor fitting) by heating with a MAPP torch I had to run through *many* WD40, heat, cool
cycles to get it off. But I think I may have actually partly fused the joint so this may not be necessary for you.
|
|
Nicodem
Super Moderator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
Besides heating, beating with a wooden hammer and WD40, another thing that sometimes help is to dripping acetone/AcOH until it gets between the joints
and then hammering/heating it. It sometimes works, especially on the alkali damaged joints. In other cases just about nothing helps.
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
well the WD didn`t even penetrate, the heating (Bunsen) didn`t help and bashing it on the bench (solid oak).
I did get a little WD to go in from the Other side (where the gas exists) using the WD40 pipe that comes with the can.
so I`ve got that sitting upside down now and keeping my fingers crossed.
I like the Acetone idea! that`s much less viscous and likely to get in.
there were Marble chips in there so it was probably last used for CO2 generation.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
Gah!!!!
it Worked, and had a much better penetrating power, and Now I have them apart Finally thanks to that a plank of wood I shaped and a BFH!
sadly it`s bady cracked (the already cracked) separator between the liquid and solid stage, so I`ll need to blow a piece of glass or make from an
already existing piece another separator (doesn`t seem to be That complicated), although it would have been nice to keep it as Original.
but at least it will now Work again! and hopefully have another 50+ years of use!
Thanks everyone for your help, I was about to half fill it with Fluorescien and just have it as an Ornament in the Living room
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
here`s the final result, the Blue wire btw, it simply to stop it re-joining again until I can get around to cleaning it properly:
![](http://myweb.tiscali.co.uk/yt2095/kipps.jpg)
this is the Broken bit, the crack at the top doesn`t show, but it IS cracked too:
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
Antwain
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 252
Registered: 21-7-2007
Location: Australia
Member Is Offline
Mood: Supersaturated
|
|
Thats a nice piece of equipment!
|
|
Ozone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
Since it wasn't mentioned, I find that the old ultrasonic cleaner/bath (sometimes in a large beaker w/acetone in the bath) is enormously helpful with
unfreezing ground glass joints.
Nice piece of glass!
Cheers,
O3
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|
Antwain
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 252
Registered: 21-7-2007
Location: Australia
Member Is Offline
Mood: Supersaturated
|
|
Really? Ive seen glass shatter in an ultrasonic when it touched other glass
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Nice Kipp's; I invite you to look into finding some teflon sleves for really important (ie expensive/ hard to replace) joints like that . I know you
may know about them but others here might not and this seems like a good chance to tell them.
|
|
Ozone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
Quote: | Originally posted by Antwain
Really? Ive seen glass shatter in an ultrasonic when it touched other glass
|
I have only seen this happen if the glass was already cracked. OTT, this seems to work fine. Usually, I'll just put the piece under water in the bath
and let it go for an hour.
Beware though as in some cases the writing/graduations on the glass can be polished off.
Cheers,
O3
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
so which technique finally worked? the WD40 or the acetone/AcOH?
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
it`s hard to say, when sprayed from the indie the WD did creep into the joint about 1/3 of the way, I cleaned all that away (as much as would come
out) and then added the Acetone, GAA mix, that almost made it trough to other side in one or 2 places within a few minutes.
it still refused to shift, so I got a plank of wood (a floor board) and cut a `(` shape into it that fit the underside of the the joint, lay the whole
thing down on packing plastic, grabbed the end with my feet and kept hitting it with a hammer and turning the kipps a little between each blow.
took about 30+ hits
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
hydride_shift
Harmless
Posts: 23
Registered: 25-7-2013
Member Is Offline
Mood: sp3 hybridised
|
|
utfse saved the day
|
|
quantumchromodynamics
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 67
Registered: 25-9-2013
Location: with much determination, nowhere in particluar
Member Is Offline
Mood: tired but still trying
|
|
crazy thing that works
Before attempting the soaking methods, I promise this works almost every time, and is easy to do.
First face the joint forward and hold the receptacle firmly. Then with a little force, not much at all, just "tink" the joint back a few times with
something like a butter knife. Then "tink" the joint from behind with the force directed forwards a few times. Finally, "tink" the joint from the left
or right a few times, but not on both sides. Nine time out of ten, the joint just falls out.
I believe if the joint is nice and round the first two steps focuses the friction into two parallel lines, and the final step focuses the friction
down to just two points.
It is a little freaky how well this little trick works.
|
|