Author: Subject: Formula of Ammonium Molybdate
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 26-7-2007 at 11:43
Formula of Ammonium Molybdate


Hello,

Can anyone tell me the formula of Ammonium Molybdate. There seems to be some confusion with different formula coming from different quarters.

Dann2
View user's profile View All Posts By User
Xenoid
National Hazard
****




Posts: 776
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline

Mood: Comfortably Numb

[*] posted on 26-7-2007 at 12:04


My copy of "Mellor's Modern Inorganic Chemistry" 1961 edition, by G.D.Parkes (don't laugh, I've had it all my life) states;

"The molybdates do not as a rule, have simple formulae such as X2MoO4, because of the readiness with which POLYmolybdates are formed. Ammonium molybdate for instance, is represented by the formula (NH4)6Mo7O24.4H2O, ie. as a derivitive of a hepta-molybdic acid. Made from acting upon molybdenum trioxide with aqueous ammonia, and allowing the solution to crystallise."

Xenoid
View user's profile View All Posts By User
agent_entropy
Hazard to Self
**




Posts: 91
Registered: 17-7-2006
Location: U.S.
Member Is Offline

Mood: No Mood

[*] posted on 26-7-2007 at 12:06


the formula for the hydrate is: (NH4)6Mo7O24 * 4H2O
F.W. 1235.86

(Taken directly from the label on a jar of the material from Fisher Scientific Company)
View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 26-7-2007 at 12:10


(NH4)2MoO4

Also

(NH4)6Mo7O24 + 4H2O

ammonium heptamolybdate tetrahydrate

[Edited on 26-7-2007 by Rosco Bodine]
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8080
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 26-7-2007 at 15:05


And to make things even more complicated, there also is an anhydrous form of (NH4)6Mo7O24, which is sold as 'molybdic acid'. The latter is a slowly soluble white powder. Once it is dissolved in water, it cannot be distinguished anymore from solutions of the 4-hydrate.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 26-7-2007 at 17:36


Hello,

Thanks for replys. My Ammonium Molybdate is EBAY stuff.
How would I find out how much Mo I have per gram?

The stuff is white lumps, quite hard, as I have to grind them down with a pestle and mortar to get them to dissolve in water.

Dann2
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 26-7-2007 at 19:01


Gravimetric is easy enough. Dissolve a weighed amount in water, add an excess of something whose molybdate is well-defined and highly insoluble (barium?), filter, dry and weigh the precipitate. Calculate based on molecular weight.

Alternately, pyrolyze to MoO3 (assumes only volatile ammonium is present), or reduce (in solution or with hydrogen, carbon, etc.) to a lower oxide or to the metal.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Ozone
International Hazard
*****




Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline

Mood: Integrated

[*] posted on 26-7-2007 at 20:00


(NH4)6Mo7O24-4H2O, correct.

A little search enginage would give:

http://www.sciencemadness.org/talk/viewthread.php?tid=7163&a...

Although... I dig the ammonium molybdate/molybdic acid bit. Amazingly vague for such a common reagent, no?

It is also quite useful for the determination of phosphate and silicate.

Cheers,

O3




-Anyone who never made a mistake never tried anything new.
--Albert Einstein
View user's profile View All Posts By User
Xenoid
National Hazard
****




Posts: 776
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline

Mood: Comfortably Numb

[*] posted on 27-7-2007 at 03:32


Quote:
Originally posted by dann2

How would I find out how much Mo I have per gram?

The stuff is white lumps, quite hard, as I have to grind them down with a pestle and mortar to get them to dissolve in water.

Dann2

Yeah! I see what you mean!

If you dissolve it in water, and then recrystallise it, you will then have the tetrahydrate for certain!

By my calculations the amount of Mo in the tetrahydrate should be 7 x 95.94 / 1235.36 which is .5436 or 54.36%

Xenoid

[Edited on 27-7-2007 by Xenoid]
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 27-7-2007 at 08:45


Oh yes - I have some of it sitting on a shelf at home here.
View user's profile View All Posts By User
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 27-7-2007 at 19:05


Hello,

It when you add a tiny amount of SnCl2 dissolved in acidified water to A.M. dissolved in slightly acid water (HCl) you get a green ppt. If you use 12% HCl to dissolve both the Ammonium Moly. and the SnCl2 you get no ppt but a nice yellow/orange clear solution.
What is the green ppt?

A.M. is used in the dying business.

Dann2
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8080
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 28-7-2007 at 09:28


Molybdenum usually occurs in oxidation state +6 in its salts. As such, it forms oxo-anions, which are colorless and your ammonium molybdate is an example of that.

Molybdenum can, however, fairly easily be reduced to a lower oxidation state (+5, +4, and even +3). When the reduction is only partial, such that most remains in the +6 oxidation state and a small amount goes to +5, then mixed-oxidation state compounds can be formed. These compounds contain (within the SAME molecule or ion) molybdenum in oxidation state +5 and +6. Such compounds have intense colors, usually blue, but they can also be black, or dark green. Search the Internet for 'molybdenum blue' and you'll certainly find information on this.

If more reductor is added, then all molybdenum goes to a lower oxidation state. With strong reductors, you can indeed go to the orange/brown compounds, which are molybdenum(III), complexed with chloride. Similar results are obtained, when powdered zinc is added to a solution of a molybdate in hydrochloric acid.