hey guys,

I am currently working on my stack for my redox flow cell. Problem is that can't find any shop online which is offering this "special" flow half cell. On the following YT clip, u can see the half cell.

https://youtu.be/u1TYDh8QRIc?t=305

I am also glad to hear other ideas of building a redox flow stack.

Kind regards,

Reaktionchamber
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2018 at 04:17


Well I will keep a close eye on this as I often planned to make one.

I live off grid with lots of 1kL tanks so no shortage of storage capacity!
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2018 at 08:38


It looks like it was made from perspex sheet.
View user's profile View All Posts By User
RustyRonny
Harmless
*




Posts: 1
Registered: 11-7-2018
Member Is Offline

Mood: Slighty Corrosive

[*] posted on 14-8-2018 at 05:34


Hi Reaktionchamber,

The half cell could likely be made from a plastic block by drilling down and then from the sides several times, the multiple holes allow the equal distribution of the electrolyte through the felt I would assume. Are you trying to make the same cell as shown in the video or another?