found stumbling through the net...
The manufacturing of TONITE
The pdf was not to get anymore but GOOGLEs rip helper utility "show as HTML" delivered it. HTML taken, converted to txt here it is attached.
Some formatting is lost but not so far to render it unreadable.
Sorry my knowledge in this kind of energetika is still much to small to decide if this is "old hat", "known but nice", "thy
bomb". A short look told me that exquisite rawmaterials are involved - stearite, starch, molasses.....
For my unknowing eyes it sounds on first sight VERY interesting - have a look.
Attachment: Tonite.txt (55kB) This file has been downloaded 1536 times
|
|
Organikum
resurrected
Posts: 2330
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Attention please!
The link works now all of a sudden, the pdf is to big to attach (1,4MB) so here the url for direct dl:
tonite.pdf 1,4MB dl here
enjoy!
|
|
Organikum
resurrected
Posts: 2330
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Ah - yes. Hm. What now?
magic rule 37 says: If you cannot convince them - confuse them!
Thats the "big reaction setup".
Thats the "standard reaction setup"
And the setup for the distillation of solids, also called "short way distillation" as this setup is to be made as near as possible to the
next beer automat. Coca Cola may sufficice but beer is superior! Pepsi? Forget it.
Thats what all have been waiting for I know it!
attached is the very interesting "Young Chemist". In russian.
Attachment: YoungChemist.djv (41kB) This file has been downloaded 927 times
|
|