Ni on charcoal catalyst.
I was surfing for information on catalysts at the hive when I came across a topic on using Ni on charcoal as a replacement for Pd, as a catalyst. I
was hoping to possibly apply it to my research in converting ammonium to HNO3 via catalyst. It could also have use as a cheap catalyst in many organic
syntheses. I figured that you guys may find it intresting. Anways heres the PDF documents.
Attachment: nickel-on-charcoal.pdf (230kB) This file has been downloaded 903 times
Vir sapit qui pauca loquitur.
|
|
NERV
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 152
Registered: 22-9-2002
Location: USA
Member Is Offline
Mood: Fluorinated
|
|
The PDF on preperation of Ni on charcoal:
Attachment: nickel-on-charcoal.preparation.pdf (73kB) This file has been downloaded 819 times
Vir sapit qui pauca loquitur.
|
|
Organikum
resurrected
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2335
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Sorry to tell, but I am quite sure that this catalyst is not useful in a ammonia to nitric acid process.
By far not active enough.
Also in most organic reactions the traditional Urushibara catalyst in it´s several ways of preparation (acidic or basic) seems preferable to me from
flexibility and ease.
I believe that Ni-hydrides will make good catalysts in future and that the zeolithes are a way to go also for the amateur experimenter.
I attached something on zeolithes - not 100% on topic but sitting on my hdd it helps nobody.
Attachment: ZEO.PDF (142kB) This file has been downloaded 977 times
|
|