[*] posted on 1-11-2017 at 05:24
Urea, OTC, CHEAP, and EASY


A week or so ago, I got about a litre of DEF (Diesel exhaust fluid) from a trucker. I measured out approximately 500ml into my vision saucepan, marked the level on the side with a Sharpie and simmered it until one third of the liquid was gone. Set it off the heat and covered it with a towel (my house is DUSTY). The next morning there was an almost solid mass of beautiful snow white urea. No filtering, no muss, no fuss!

After a couple days drying at room temp on a paper towel covered plate the yield was 155gms. I wish I had a functional camera at the moment so I could post a picture!

The jug that it came from, TRCair UltraPure DEF, contains 9.46 litres full,giving an EASILY obtainable yield of almost 3 kilos (2923gms) of Urea. This product is available at Tractor Supplu stores in my area (Texarkana, USA) for $8.99, making the cost $3.00 a kilo for pure Urea!

This is a big plus for me, as I was obtaining urea from fertilizer and it comes in prills dyed green. Big pain in the ass requiring multiple recrystallizations to get rid of green dye, and still never comes out snow white. I had used it for Chemplayers Citrazinic Acid synth and got crappy results. Going try again with this BEAUTIFUL snow white Urea!




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8037
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 1-11-2017 at 07:32


Sounds interesting. What is diesel exhaust fluid? I never heard of this. Maybe it is something unknown where I live, but if you can make urea from this easily then that would be interesting for me as well.

Where I live, you can buy urea prills, but they are very dirty. If you add them to water, you get a turbid liquid with a lot of pale yellow/brown scum on it and it is a pain in the ass to make pure crystalline urea from this. I always end up with some pasty/sticky off-white stuff. It seems like the urea is mixed with some greasy or oily stuff which is very hard to separate. Probably this stuff is added to the urea to keep it more or less free flowing, also when stored in a cold and humid barn.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Melgar
Anti-Spam Agent
*****




Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline

Mood: Estrified

[*] posted on 1-11-2017 at 08:10


Urea solution can be sprayed into diesel exhaust to neutralize NOx vapors. Tractor trailers are too big to have catalytic converters, after all.



The first step in the process of learning something is admitting that you don't know it already.

I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 1-11-2017 at 08:47


In the UK you tend to find the empty containers discarded at lay bys and lorry parking areas. Until I looked it up I did wonder why diesel engines needed urea. Yes it could be a cheap source of pure urea. You can ocasionaly see big dump bags of urea at farms or see them being transported to farms. The urea in them looks pure white a coarse powder.

Don’t forget the bulk de-ices. They are starting to appear in the shops.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3032
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 1-11-2017 at 11:55


@Woelen; DEF is sold in the Netherlands as AdBlue, for around 1,50 a liter.
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 1-11-2017 at 12:01


This is the stuff that was added to cars to pass the emission tests, alot of cars have/had a tiny tank of it, when in a test the ecu turns it on and the emissions are lowered. I never understood why this isnt a main feature, except on the TV program about VW being prosecuted, they mentioned damage to engines because the exhaust gas goes back into the engine first, via something called a EGR or something

Ok I got it very slightly wrong, this explains it, apparently alot of cars have this but few people I assume know about it, the stuff is called ad blue in the UK. Anyone in the UK will know the VW story

https://www.newscientist.com/article/dn28240-how-did-volkswa...

[Edited on 1-11-2017 by NEMO-Chemistry]
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1708
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 1-11-2017 at 13:18


"Made from high purity urea and deionized water
Contains no chemical additives or other compounds that could cause SCR system failure
Meets the quality standards established by the ISO-22241-1 for Diesel Exhaust Fluid
Certified by the American Petroleum Institute"
http://www.autozone.com/miscellaneous-cleaners-and-degreaser...

Pour it on your pants ...
DEF - PEAK BlueDEF (Diesel Exhaust Fluid) | PEAK Commercial and Industrial
https://www.youtube.com/watch?v=E8Mn0HyBWCI

How Does DEF (Diesel Exhaust ) Fluid Work & Is it Really Pee? The Chemistry of Cars Ep. 1
https://www.youtube.com/watch?v=NPM40ey1OHQ

[Edited on 1-11-2017 by Morgan]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 1-11-2017 at 13:28


I wasn't aware there was a urea shortage among amateur chemists.
View user's profile View All Posts By User
The Volatile Chemist
International Hazard
*****




Posts: 1981
Registered: 22-3-2014
Location: 'Stil' in the lab...
Member Is Offline

Mood: Copious

[*] posted on 1-11-2017 at 15:02


Quote: Originally posted by unionised  
I wasn't aware there was a urea shortage among amateur chemists.

Indeed...It took me a bit to source some, but I found a few local sources for urea and I don't imagine running out. Looking forward to some amide experiments soon, hopefully...




View user's profile Visit user's homepage View All Posts By User
Vosoryx
Hazard to Others
***




Posts: 282
Registered: 18-6-2017
Location: British Columbia, Canada
Member Is Offline

Mood: Serial Apple Enjoyer

[*] posted on 1-11-2017 at 15:25


Quote: Originally posted by unionised  
I wasn't aware there was a urea shortage among amateur chemists.


Yeah i've never had trouble finding it, albeit slightly more expensive than this source. (Although likely more pure)
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 1-11-2017 at 15:57


That is one source of urea also another one is doller store ice packs the cheapest ones have urea prills in it



View user's profile View All Posts By User
Vosoryx
Hazard to Others
***




Posts: 282
Registered: 18-6-2017
Location: British Columbia, Canada
Member Is Offline

Mood: Serial Apple Enjoyer

[*] posted on 1-11-2017 at 16:32


Quote: Originally posted by symboom  
That is one source of urea also another one is doller store ice packs the cheapest ones have urea prills in it


Yeah, I use the instant cold packs. They're dirt cheap where I live.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1708
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 1-11-2017 at 17:34


On eBay now ...

5LB. UREA(46-0-0) 46% Nitrogen Fertizlizer Gold Refining Aqua Regia 100% Soluble

"This is 99+% urea for use in gold recovery process, fertilizer and neutralizing acid in aqua regia. It is a colorless, odorless solid, although its gives off a strong ammonia smell in the presence of water. It is highly soluble in water and practically non-toxic. Dissolved in water it has a neutral ph. It is a convenient source of nitrogen when used as fertilizer."
Price:US $11.45

50 pounds - $18.99
https://standishmilling.com/catalog/fertilizer/50-lb-46-0-0-...

$16.99
https://www.farmstore.com/product/46-0-0-urea-fertilizer-50-...

[Edited on 2-11-2017 by Morgan]
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 4-11-2017 at 04:45


$9.00 for 3 kilos of snow white urea seems like a deal to me



"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
The Volatile Chemist
International Hazard
*****




Posts: 1981
Registered: 22-3-2014
Location: 'Stil' in the lab...
Member Is Offline

Mood: Copious

[*] posted on 4-11-2017 at 20:18


Quote: Originally posted by arkoma  
$9.00 for 3 kilos of snow white urea seems like a deal to me

True. And besides, it's OTC, and easily available to you.




View user's profile Visit user's homepage View All Posts By User
Morgan
International Hazard
*****




Posts: 1708
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 5-11-2017 at 04:58


Tidbits
http://www.indexmundi.com/commodities/?commodity=urea
http://www.farmfutures.com/story-weekly-fertilizer-review-0-...


View user's profile View All Posts By User

  Go To Top