Oxalic acid dihydrate is marketed as a rust remover for use in the home. Sold in hardware stores and online also as a wood bleach.
Give it a try, as you can always find other uses for H2C2O4 as many of its salts are conveniently insoluble.
To be honest, have not used it to dissolve Fe2O3 and don't quite understand have the yellow insoluble FeC2O4 is easier to remove.
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
The oxalate anion acts as a very good ligand for the Fe3+ (and may be 2+ too) cation, it binds to the cation and makes it stay in the solution as
Fe(C2O4)3 3-.
|
|
franklyn
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline
Mood: No Mood
|
|
How to make Ferrofluid
www.youtube.com/watch?v=LlQw9dfexBQ
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Thanks for the bump, franklyn!
As you can see, my ferrofluid was also non-spiking and acted just like the OP's. I'd like to retry this at some point, and I'll take into
consideration the suggestions used here. I suspect the oleic acid was my problem as well.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) |
To be honest, have not used it to dissolve Fe2O3 and don't quite understand have the yellow insoluble FeC2O4 is easier to remove.
|
With excess oxalic acid ferric ions from the stable and highly soluble trisoxalotoferrate complex:
Fe(Ox)<sub>3</sub><sup>3-</sup>. Slightly surprisingly it's green and a bit fluorescent too. Needs acid conditions because
alkalinity destroys it because Fe(OH)3 is more insoluble than the complex is stable. There's a nice synth of K3Fe(Ox)3 on this board somewhere.
|
|
uzaymaymunu
Harmless
Posts: 34
Registered: 26-2-2012
Location: turkey
Member Is Offline
Mood: No Mood
|
|
Finally spiking. But it's not good quality. Here is the video and picture:
http://uzaymaymunu.blogspot.com/2012/04/ferromanyetik-akskan...
|
|
Oggas
Harmless
Posts: 8
Registered: 10-5-2011
Member Is Offline
Mood: No Mood
|
|
I might have missed something while reading the thread, but i do not understand what the oxalic acid is for, is it supose to be used as a surfacant in
place of the oxalic acid?
Also, does anyone know a good source for oleic acid or something that could be used to replace it since i had not had any luck acquiring it so far.
Thanks.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Olive oil. Olive oil is essentially the triglyceride of oleic acid.
Saponify the oil with NaOH or KOH (loads of information on quantities to use on various DIY soap sites). Now you have the crude salt (soap) of oleic
acid.
Hydrolyse this with a sufficient quantity of a dilute solution of a strong acid. The oleic acid separates out (it's not water soluble). Wash and dry
and you've got crude oleic acid.
[Edited on 17-5-2012 by blogfast25]
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Will magnetite powder from a pottery store work to make ferrofluid? I don't see why it shouldn't, but I don't quite know the particle size.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
uzaymaymunu
Harmless
Posts: 34
Registered: 26-2-2012
Location: turkey
Member Is Offline
Mood: No Mood
|
|
This is useful.
Attachment: Charles_Prep.pdf (283kB) This file has been downloaded 488 times
uzaymaymunu.blogspot.com
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Almost certainly not. I think the best result you could hope for there is a fluid that weakly responded to magnetic fields, but certainly not
something that formed spikes.
When making ferrofluid the particle size is *very* important. The stuff from the pottery store would just have been ground up, or ball milled if you
are lucky. I understand the easiest way to get a small particle size is to precipitate the iron oxide out (See MrHomeScientist's video). I have also
heard that some people have had success by using the particles on magnetic tapes, so if you have a bunch of those you might want to look into it.
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1701
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
I've been looking at ferrofluids this week, and I'm ready to blow a gasket over the complete lack of detail in any procedure available online. Some
lists quantities of FeCL2/Cl3-solution without listing concentrations, most don't even bother listing that. For fucks sake, why hasn't anyone made a
procedure that produces spiking fluids with some repeatability?
We're not banging rocks together here. We know how to put a man back together.
|
|