Making refractory from CaO ?


I have some CaO and want to make firebricks in which I can deploy an electric arc with a 150A DC welder.
Any other refractory melts and vaporizes (yes, I know, CaO too, but slower due to higher mp, so they last longer).

Is there a binder (clay ?) with which I can make small bricks from CaO powder ?
View user's profile View All Posts By User
Jstuyfzand
Hazard to Others
***




Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline

Mood: Learning, Sorta.

[*] posted on 2-10-2016 at 01:28


You would be better off buying some proper bricks and carving a reactor from it, a la Grant Thompson.