Author: Subject: Looking for help building my down's cell
b_d_Dom
Harmless
*




Posts: 32
Registered: 27-10-2006
Location: Canada
Member Is Offline

Mood: No Mood

[*] posted on 27-10-2006 at 15:28
Looking for help building my down's cell


I already know all the physics and chemistry behind but I am looking for some advice from people who have actually built them and can offer some construction tips

Right now I am looking for a suitable heat source, preferably electric and it must get at least 700 C, I am using a NaCL CaCl mixture

EDIT: I searched this site but found few actual building instructions, mostly just more chemical formulas

[Edited on 27-10-2006 by b_d_Dom]
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 27-10-2006 at 15:32


Have you searched this site to see what work may already have been done on this subject?



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 27-10-2006 at 16:28


I've built one before, see my references to it in the thread entitled "Hot electrochemical sodium". Also, 700*C is way too hot. Your salt will volatilize. Please research more. I can send you an email if you like...



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
b_d_Dom
Harmless
*




Posts: 32
Registered: 27-10-2006
Location: Canada
Member Is Offline

Mood: No Mood

[*] posted on 28-10-2006 at 18:41


Ya an email would be great! I sent you an U2U with my address.

Also because I am using the 40% NaCl + 60% CaCl2 mix I would need a minimum of 580 C, and 700 C would be preferable so I can build a larger machine.