kadriver
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 7-11-2012
Location: United States
Member Is Offline
Mood: Thankful
|
|
Recovering Gold From Used Filter Papers - VIDEO
My title says platinum, but there was so little of it that I just added it to my stock pot.
Also, this was my first time processing this type of material so I didn't know what to expect.
https://youtu.be/GYDGOSDPTxc
Thank you!
kadriver
Youtube channel - sreetips
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Your videos (plus others and members here) have been my inspiration to recover gold, for 'fun'/learning only, not at all at your scale,
You got 4x more gold from your 'waste' filter papers than I have recovered in total ![:P](./images/smilies/tongue.gif)
not interesting for a video but
because of the tiny amounts, rather than filtering most stages just need patience, weeks of it, but much less 'waste'.
P.S. judging by the number of containers I guess you already use time to separate out solids ... d'oh
Even with the tiny ammounts of gold that I have experimented with, I can see the attraction of this element, useful but
I especially like the look of (presumed) almost pure gold in solution, a wonderful yellow, gold lust inducing.
[Edited on 23-2-2016 by Sulaiman]
[Edited on 23-2-2016 by Sulaiman]
|
|
|