crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
Bismuth oxide reduction
Hello,
I have been growing bismuth crystals a while ago and beside nice hopper crystals I also got some bismuth oxide from melting.
Is there a simplier way to reduce that oxide to elemental bismuth than reducing it with carbon under big temperatures without presence of oxygen?
Thakns for answer.
[Edited on 31-1-2016 by crystal grower]
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
You can dissolve the bismuth oxide in hydrochloric acid, and then reduce it with aluminum foil, yielding a fine black powder of bismuth metal. This
can then be dried and washed again with dilute HCl to remove excess aluminum, as bismuth will not dissolve in it.
|
|
crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
Quote: Originally posted by zts16 ![](images/xpblue/lastpost.gif) | You can dissolve the bismuth oxide in hydrochloric acid, and then reduce it with aluminum foil, yielding a fine black powder of bismuth metal. This
can then be dried and washed again with dilute HCl to remove excess aluminum, as bismuth will not dissolve in it. |
Thanks for answer, I will definitely try it .
|
|
Tdep
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Expect to run into serious difficulty when trying to melt bismuth powder back into a lump. Despite it seeming easy because of the low melting point,
the powder has always oxidized before it melts for me.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Quote: Originally posted by Tdep ![](images/xpblue/lastpost.gif) | Expect to run into serious difficulty when trying to melt bismuth powder back into a lump. Despite it seeming easy because of the low melting point,
the powder has always oxidized before it melts for me. |
I guess you need either a suitable slag or an argon environment.
Suggestions for the former anyone?
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Sodium hydroxide worked when I was melting cadmium powder. The trick is to have a lot of metal powder and just enough flux to cover the surface, it
seems.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
A low melting flux, like a soldering/brazing flux?
Teflon? MP = 327 C
[Edited on 1-2-2016 by blogfast25]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by elementcollector1 ![](images/xpblue/lastpost.gif) | Sodium hydroxide worked when I was melting cadmium powder. The trick is to have a lot of metal powder and just enough flux to cover the surface, it
seems. |
Bismuth is amphoteric: chances are there will be reaction between molten Bi and molten NaOH.
Paraffin wax? BP > 370 C. Melt wax, add Bi powder until wax solidifies. Re-melt wax, add more Bi-powder util wax re-solidifies. Repeat until all
Bi-powder added and T > 280 C. Cool and find puddle of frozen Bi, neatly protected by paraffin. Live happy ever after. ![:D](./images/smilies/biggrin.gif)
See: https://books.google.co.uk/books?id=kaa2qeFRXmUC&pg=PA62...
Stearic acid: BP = 361 C.
[Edited on 1-2-2016 by blogfast25]
|
|
crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
Thanks everyone for answers.
I used to compress powders when I needed to melt them, but I will try to melt it with parafin as u said.
It seems to be simplier way.
[Edited on 1-2-2016 by crystal grower]
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 513
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by crystal grower ![](images/xpblue/lastpost.gif) | Hello,
I have been growing bismuth crystals a while ago and beside nice hopper crystals I also got some bismuth oxide from melting.
Is there a simplier way to reduce that oxide to elemental bismuth than reducing it with carbon under big temperatures without presence of oxygen?
Thakns for answer.
[Edited on 31-1-2016 by crystal grower] |
According to Nile Red you can simply heat the bismuth oxide and it will decompose into oxygen and bismuth metal.
See this video, at around 4 minutes 45 seconds.
https://www.youtube.com/watch?v=grpSfjUImUs
|
|
crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
Of course but it must be in inert atmosphere as far as I know.
Or am I wrong ?
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
I would consider hydrogen gas atmosphere, which you may more inexpensively and easily generate.
[Edit] Downside, H2/air presents an explosion hazard.
[Edited on 1-2-2016 by AJKOER]
|
|
bismuthate
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline
Mood: self reacting
|
|
It seems unlikely to me that the two would react. What would you believe the reaction would yield?
Also any gas tank for welding or a stream of dry hydrogen should work for an atmosphere. Heck, even CO2 might work, but I'm not sure about that one.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Per Atomistry on Bi2O3 (link: http://bismuth.atomistry.com/bismuth_trioxide.html ) to quote:
"The trioxide does not decompose when heated to 1750° C. It is reduced, partially or completely, by a number of reducing agents, such as hydrogen,
carbon, carbon monoxide, silicon, sodium, potassium, methane, ammonia, ammonium chloride, potassium cyanide, aluminium carbide, and an alkaline
stannous solution. "
where the use of heated NH4Cl or an alkaline stannous solution seem interesting. Note, the result may just be a partial reduction to BiO.
If BiO is formed, to quote Atomistry on BiO:
"It is easily reduced to metal by heating on a charcoal block, or in a current of hydrogen or carbon monoxide; reduction in hydrogen takes place at
300° to 310° C., and in carbon monoxide begins at about 250° C."
Also:
"It is converted to metal by reaction with aqueous potassium hydroxide alone"
Link: http://bismuth.atomistry.com/bismuth_monoxide.html
[Edited on 1-2-2016 by AJKOER]
|
|