Bakelite colour
Guys,how is bakelite marbled?I'm talking about that mixed brown and black colours,I searched on google and found this "marble" name for this black and
brown...Here's a picture:
http://www.first-s-mart.eu/images/20130228/954/1.JPG
|
|
Dr.Bob
International Hazard
Posts: 2685
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
They can add a random mixture of dyes or colored resins to the material when it is molded. Similar to making artificial countertops (corian,
silastone, etc) with mix of diffent colored resin particles and molding under heat and pressure.
|
|