drying white phosphorus
I will need to dry a small amount of white P just prior to its use. I store my white P under water. Below is my plan for doing this. Please
critique this plan. If you know a better way please explain:
Drying of the White Phosphorus
The phosphorus is currently stored under water. Any entrained water must be removed prior to the time of use.
1. Place ~ 25ml of acetone in a 50ml Erlenmeyer flask.
2. Add ~1g of P2O5. Cork and swirl.
3. Pre-weigh the Erlenmeyer flask with the acetone, P2O5, and cork.
4. Cool the phosphorus in water to 5-10°C.
5. Remove ~2g of phosphorus, pat it dry on a paper towel, and place it in the Erlenmeyer flask.
6. Reweigh the flask and record the weight of phosphorus added.
7. Swirl the flask and set aside for an hour with occasional swirling
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
gdflp
Super Moderator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline
Mood: Staring at code
|
|
The only possible issue I see with this plan is that the phosphorus could ignite as you are taking it out of the acetone. If that was the case, then
you could get quite a surprise as the acetone ignited. As long as you're prepared for this, I think that it should work fine. Would drying the
phosphorus with concentrated sulfuric acid, then rinsing a few times in a dry organic solvent to remove the excess sulfuric acid be feasible? A
combination of the two might work well, as the sulfuric acid could remove most of the water, while the phosphorus pentoxide could remove the last
traces. Just a thought.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I will be transferring the P directly from the acetone to 100 mls of chloroform, so it will not have a chance to heat up.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
FENIAN FIRE!!!
Put a drop of the white P solution on something like a piece of paper- Leave on a fireproof surface. Wait for the solvent to evaporate...
[Edited on 7-2-2015 by Bert]
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
The basis of my method is that P does not react with nor dissolve in acetone.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
But it DOES dissolve in chloroform, about 1g:40ml.
I understand the acetone should not dissolve the P. But be careful about any little splashes of the chloroform solution, white P in carbon disulfide
or chloroform was used as a sabotage incendiary mixture. Casualy pour it on something, walk away. A bit later there is a white P fueled fire.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Hawkguy
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 326
Registered: 10-10-2014
Location: British Columbia (Canada eh!)
Member Is Offline
Mood: Body is Ready
|
|
Purge the flask with the WP using Carbon Dioxide. That should prevent whatever.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Yes, that is my purpose for using chloroform in the synthesis to follow.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Dan Vizine
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 628
Registered: 4-4-2014
Location: Tonawanda, New York
Member Is Offline
Mood: High Resistance
|
|
I'd simply put the P in the CHCL3 and use azeotropic distillation (with a Dean-stark that returns the BOTTOM layer).
Protect from light!. I haven't looked it up in some time, but the heating alone shouldn't cause much change.
Where applicable, azeotropic drying is the method of choice for economy and, often, efficiency.
Lots of solvents have immiscible water azeotropes,.... methylene chloride, chloroform, toluene, xylene, and many more.
[Edited on 8-2-2015 by Dan Vizine]
"All Your Children Are Poor Unfortunate Victims of Lies You Believe, a Plague Upon Your Ignorance that Keeps the Youth from the Truth They
Deserve"...F. Zappa
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Dan Vizine:
That does look like a good way to remove water. So I should keep distilling until the bp rises to that of pure CHCl3, correct?
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Hennig Brand
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1284
Registered: 7-6-2009
Member Is Offline
Mood: No Mood
|
|
How about putting the wet sample of P in a drying tube and passing a stream of inert gas through until dry (if you have access to bottled inert gas it
should dry very fast). Or, maybe generate an appropriate gas and collect it using a pneumatic trough or some other apparatus. The P sample to be dried
could be placed in the vessel with the gas along with a suitable desiccant. I suppose for that matter the P could be stored in inert gas as well.
"A risk-free world is a very dull world, one from which we are apt to learn little of consequence." -Geerat Vermeij
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Here's what I think you should do:
-Place the phosphorous in a 2-necked flask along with some acetone or other low-boiling water miscible solvent. One neck of the flask should have a
vacuum take-off adapter, and the other should have an addition funnel
-Using a vacuum pump, evaporate off the acetone/water, leaving the dry phosphorous behind. Then turn the vacuum off and open the addition funnel. The
chloroform should be sucked sown by the residual vacuum to cover the phosphorous, without the phosphorous ever having been exposed to air.
This method has the advantage that everything happens in one flask, and the phosphorous never gets the chance to ignite, since it is always either wet
or covered with a liquid.
|
|
Hennig Brand
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1284
Registered: 7-6-2009
Member Is Offline
Mood: No Mood
|
|
"Purification of Laboratory Chemicals" simply says to dry under vacuum.
"A risk-free world is a very dull world, one from which we are apt to learn little of consequence." -Geerat Vermeij
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2166
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Under vacuum sounds safer, no oxygen.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
You guys are coming up with some good ideas. Thanks.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|