Eclectic
National Hazard
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
Carboxymethylcellulose
I've got some weed killer which apparently 20% carboxymethylcelulose judging from the slimy, viscous mess produced when I dissolved it in water. Does
anyone know a way to denature, coagulate, or otherwise get rid of the viscous properties of this stuff? I'd like to recover the sodium metaborate and
sodium chlorate that make up the rest of the weed killer, so any fixes using acids are out.
|
|
vulture
Forum Gatekeeper
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Don't copper ions "dissolve" cellulose compounds?
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
chemoleo
Biochemicus Energeticus
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Try biological washing powders...which should contain cellulase, the enzyme. Maybe you can digest it such that the viscosity becomes managable. Be
sure to run at at 40 deg C or wahtever, whatever the washing powder specifies.
Else...centrifugation may be another method, for compacting the goo.
[Edited on 27-6-2006 by chemoleo]
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
Eclectic
National Hazard
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
I'm getting some crystallization from what I strained through a sieve. Maybe just patience is the answer. I'll dilute the mess a little more and just
let is slowly evaporate, then sieve out the large crystals.
Exploding pants, anyone?
|
|
unionised
International Hazard
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
"Try biological washing powders...which should contain cellulase, the enzyme." I doubt that. Has anyone seen a washing powder labeled "Warning: may
dissolve cotton"?
|
|
Eclectic
National Hazard
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
Nevermind, I think the viscosity was from microcrystals. The 20% inert material may just be salt or sodium carbonate. 5 lbs of the stuff seems to
dissolve fairly well in 2 gallons of water. I initially tried 3 quarts. I'll just slowly evaporate for fractional crystalization.
|
|