Author: Subject: Lowest melting point alkali carbonate or alkali carbona eutectic
akinmad
Hazard to Others
***




Posts: 245
Registered: 24-7-2003
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2005 at 15:30
Lowest melting point alkali carbonate or alkali carbona eutectic


Dear Friends,
I hope this is the correct section for this. Recently I am researching the molten carbonate fuel cells. This type of fuel cells are the most robust fuel cells with respect to CO poisoning. However their main disadvantage is they have to be heated to operating temperature (i.e. their melting point) before they produce electricity. All alkali carbonates I am researching have high melting points. Consequently, I am looking for a low melting point alkali carbonate or alkali carbonate eutectics. Any ideas? Regards.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3245
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 3-11-2005 at 19:57


2nd result on google searching "Molten Salt Database" was the hit I was looking for.

http://ras.material.tohoku.ac.jp/~molten/molten_ps_query1.ph...

Give it a shot.




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
akinmad
Hazard to Others
***




Posts: 245
Registered: 24-7-2003
Member Is Offline

Mood: No Mood

[*] posted on 4-11-2005 at 11:44


Quote:
Originally posted by BromicAcid
2nd result on google searching "Molten Salt Database" was the hit I was looking for.

http://ras.material.tohoku.ac.jp/~molten/molten_ps_query1.ph...

Give it a shot.

Thank you. I had previously visited that link but it does not give melting points (or am I missing something?). Regards
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 4-11-2005 at 14:35


Pretty close, you wanted this.
http://ras.material.tohoku.ac.jp/~molten/molten_eut_query1.p...

I find:
System: KCl-K2CO3-Na2CO3, Mol %:42.5-43.3-18.1, Temp: 558 C
System: K2CO3-Na2CO3 , Mol %: 38.5-61.5, Temp: 695 C
System: K2CO3-Li2CO3-Na2CO3, Mol %: 26.8-42.5-30.6, Temp: 393 C

Tim

[Edited on 11-4-2005 by 12AX7]




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Texium
Administrator
Thread Moved
19-11-2023 at 10:49

  Go To Top