formation of ALUM
Why is Sulfuric Acid used to Neutralize
KAl(OH)4 Rather than HCl or HNO3, thanks for the assitance.
Fietts
fietts
|
|
DeAdFX
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 339
Registered: 1-7-2005
Location: Brothel
Member Is Offline
Mood: @%&$ing hardcore baby
|
|
Alum is a synonym for KAl(SO4)2. It is a double salt of Aluminum and Potassium Sulfate.
http://mineral.galleries.com/minerals/sulfates/alunite/aluni...
and http://www.chemicalland21.com/arokorhi/industrialchem/inorga...
For verifcation...
If you neutralized KAl(OH)4 with a different acid you would not end up with alum but a different aluminum/potassium salt + H2O
|
|