Would anyone help me on, What material should i put in commercial microwave for the liquid sodium hydroxide?
And would anyone help me which company may provide me that microwave and NaOH safe apparatus.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I really don't understand your question.
Sodium hydroxide is a solid under normal circumstances. Although it does dissolve in water to form a solution.
I am not sure why you would put sodium hydroxide in a microwave oven.
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
quick assumption here, but, are you trying to microwave solid NaOH until it fuses? w/o using metal because of oven sparks, and w/o glass because NaOH
will eat through it while molten and no plastic because of fused salt temp? cause that is not so easy off the top of my head.
please elaborate on your question in more than two sentences. if your trying to melt it, maybe a silver or nickle crucible and a bunsen burner are in
order. but I did find this also: http://web.ornl.gov/info/reports/1956/3445603500995.pdf
" Magnesium oxide is not only chemically stable in fused sodium hydroxide but is also quite insoluble. In corrosion tests, Steidlitz and Smith4 found
that single-crystal specimens of magnesium oxide in a large excess of anhydrous sodium hydroxide at 800°C. decreased in thickness by less than 0.001
in. in 117 hr "
[Edited on 21-10-2014 by violet sin]
|
|
Little_Ghost_again
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 985
Registered: 16-9-2014
Member Is Offline
Mood: Baffled
|
|
clay flower pots work ok, glazed high temp ceramic also is ok, but the molten stuff is pretty nasty andmy microwave didnt do too many batches before
something inside got eaten.
how much do you need?
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
If you just need to melt it, use a regular heat source and a nickel crucible (I got mine from Elemental Scientific).
|
|