what is the hydrate of ammonium nitrate at room temp
i cant find it any were i can't even find any hydrates of ammonium nitrate
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
I've warned you before, put more effort in your posts and make them coherent!
Next time is sanction time.
Now what the hell are you trying to say anyway?
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
kclo4
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline
Mood: No Mood
|
|
i am asking what is the maximum hydrate of ammonium nitrate at room temperature
sorry for being ignorant
|
|
hodges
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline
|
|
I believe that since ammonium nitrate is hygroscopic, it will absorb an indefinite amount of water from the air.
|
|
JohnWW
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
Ammonium nitrate crystallizes with no water of crystallization, at any temperature. Neither the ammonium nor the nitrate ion hydrogen-bond water
molecules sufficiently strongly. There are, however, two different crystalline forms, one of which (alpha, tetragonal) crystallizes at -16 to 32ºC,
and the other (beta, monoclinic) at 32ºC to 84ºC. Both decompose explosively at 210ºC.
The only nitrates that crystallize with water of crystallization are those in which the H2O is bonded as a ligand to the metal cation sufficiently
strongly, e.g. Cd(NO3)2.4H2O, Ca(NO3)2.4H2O, Cu(NO3)2.3H2O and Cu(NO3)2.6H2O, Fe(NO3)2.6H2O, Fe(NO3)3.6H2O, Ni(NO3)2.6H2O, Zn(NO3)2.6H2O,
Al(NO3)3.9H2O, Bi(NO3)3.5H2O, LiNO3.3H2O, Mn(NO3)2.6H2O, Hg2(NO3)2.2H2O. Most other metal nitrates are anhydrous.
[Edited on 2-4-2005 by JohnWW]
|
|
MadHatter
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1333
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
NH4NO3
Kclo4, what references are you looking at ? I see no hydrate versions of ammonium
nitrate in any of my CRCs. I have the 52nd, 62nd, and 81st editions. If you haven't
already done so, go to a used book store or eBay and find an edition. If you can't afford
it, local libraries tend to have an edition or 2 on hand. BTW, I paid only $15(USD) for
the 52nd edition at a local used book store.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
BASF
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
In case you are needing this info for stoicheometric calculations you might also consider the big amount of adsorbed water. I think this can be very
well in the magnitude of 50% of the total weight ... but this is very difficult to just calculate
|
|