Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Lightning Rod
This was an interesting effect of lightning on a carbon fiber fishing rod. One time I used a propane torch on a golf club made of carbon fiber to melt
off the binder. The fibers just sort of glowed after all the low temperature material was burned off.
https://www.youtube.com/watch?v=PCRguPMjXLw#t=21s
http://imgur.com/gallery/F1S8M
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
''lightning struck the rod first''
recalling to have heard that lightning does not come from the sky but rather from the ground (in this case the water) then goes upwards to the skies
ohwell i could be wrong, its the news after all (!)
pretty interesting story tho, seems... very weird...
wonder what the material would be.. it would still be carbon, if it was carbon.. but surely something happened to it
|
|
Chemosynthesis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1071
Registered: 26-9-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Antiswat ![](images/xpblue/lastpost.gif) | ''lightning struck the rod first''
recalling to have heard that lightning does not come from the sky but rather from the ground (in this case the water) then goes upwards to the skies
|
I've heard it's even more variable than this answer for general public consumption would bely, but here it is claimed "both."
https://www.nssl.noaa.gov/education/svrwx101/lightning/faq/
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Shortest answer is it doesn't matter if the lightning starts at the ground or the cloud. The current travels through the object and possibly the
person. It doesn't matter much to the dead guy if it started on the ground or in the sky.
|
|