Iodine from Copper I iodide?
I recently acquired a 50g tamper sealed bottle of Copper I iodide, labeled as 99.999% pure.
How would I isolate elemental iodine from it? Is it similar to isolating iodine from alkali metal iodide? Using sulfuric acid, or HCl and hydrogen
peroxide?
Finally one thing confuses me, the NFPA rating for the copper iodide on the bottle is 101 (health, flam., reactivity) but on the wiki page the rating
is 110.
http://en.wikipedia.org/wiki/Copper%28I%29_iodide
which is correct?
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
I doubt it would be flammable.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
It seems that the chemical supplier is much more likely to have the proper information on it than Wikipedia is.
|
|
numos
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 269
Registered: 22-2-2014
Location: Pasadena
Member Is Offline
Mood: No Mood
|
|
Ok thanks, that's what I though. Any ideas on Iodine isolation? I originally bought this to make (Cu Py3)I shown in nurdrage's video,
https://www.youtube.com/watch?v=8jDFx7yeBvw
but there's got to be more than that!
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by numos ![](images/xpblue/lastpost.gif) | I recently acquired a 50g tamper sealed bottle of Copper I iodide, labeled as 99.999% pure.
How would I isolate elemental iodine from it? |
DON'T!! Don't waste such a precious chemical to pursue another that is so easy to prepare (NaI + H2O2, for instance). You've got a 5N compound there,
ferchr*ssakes!
|
|
numos
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 269
Registered: 22-2-2014
Location: Pasadena
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by blogfast25 ![](images/xpblue/lastpost.gif) | Quote: Originally posted by numos ![](images/xpblue/lastpost.gif) | I recently acquired a 50g tamper sealed bottle of Copper I iodide, labeled as 99.999% pure.
How would I isolate elemental iodine from it? |
DON'T!! Don't waste such a precious chemical to pursue another that is so easy to prepare (NaI + H2O2, for instance). You've got a 5N compound there,
ferchr*ssakes! |
I was confused by this until I looked up the price of Copper I iodide on Sigma Aldrish... this quantity would cost nearly $260. The guy I bought it
from was an idiot... I paid $18 for the bottle, hence not feeling bad about using it. I will keep it tamper sealed for now.
Excuse my ignorance, but what does 5n mean?
and THANK YOU for the warning, I would have thrown $200 down the drain. ![:o](./images/smilies/shocked.gif)
[Edited on 3-24-2014 by numos]
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
99.999%
nearly broke my balls there
i suppose if you were to use it you could POSSIBLY use ascorbic acid as they tend to break copper salts down into metallic copper at some point, but i
think you would need the iodine to be oxidized aswell still
it seems that CuI2 can be made by CuSO4 + KI simply, this would be easy to thereafter seperate out and perhaps be possible to make into copper and
iodine from the dry product?
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by numos ![](images/xpblue/lastpost.gif) | Excuse my ignorance, but what does 5n mean?
and THANK YOU for the warning, I would have thrown $200 down the drain. ![:o](./images/smilies/shocked.gif)
[Edited on 3-24-2014 by numos] |
99.999 % = 5 nines = 5N
Now go and sell that stuff off in small amounts and make a tidy packet!
|
|