Additives for water shaker bath


I have a water shaker bath (20 C) that gets alot of red iron corrosion, the metal looks like stainless (I will confirm later)

after cleaning

would adding K2CrO4 and or Na2MoO4 help prevent this

how much would I add 100ppm of each?

and would it be wise to adjust the pH aswell to alkaline or acid state
View user's profile View All Posts By User
feacetech
Hazard to Others
***




Posts: 163
Registered: 12-2-2007
Member Is Offline

Mood: No Mood

[*] posted on 2-5-2013 at 14:17


Hmmm scrap that after cleaning thers no visable corrison on the metal surfaces, its is probly just a brown bacterial sludge and built up tds from not being drained frequently enough.