Author: Subject: Melting MgO with electric arc is EASY !!
metalresearcher
National Hazard
****




Posts: 737
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 19-4-2012 at 12:31
Melting MgO with electric arc is EASY !!


With an electric welder I made an arc which melted MgO rods like plastic ....

<iframe sandbox width="760" height="465" src="http://www.youtube.com/embed/AHAUHIOD_5Y" frameborder="0" allowfullscreen></iframe>
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 20-4-2012 at 06:26


That's neat. Perhaps you can make a MgO crucible.