Containers
I am trying to figure out what to use to hold my concentrated H2SO4. Will HDPE be alright? I have these nice big bottle that I can get from work,
they're empty Javel bottles...Wash them out, and boom, not bad? Is HDPE an all around acid/base resistant material? OR are their things that I
should not add to the HDPE. I should add that these containers are white, not clear, if this at all bears any significance. I recall having put some
H2SO4 (not concentrated) in HDPE which was a yellow plastic, and the H2SO4 turned it slightly black. Do you think I'd have the same problem with
the white containers? I don't want to contaminate my juice.
What does everyone else use to hold their fluids/chemicals? Nothig fancy I suppose, but I'd like to hear whatcha got.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Why not use glass? Like huge 1L cookie/mayo jars or something.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
I am a fish
undersea enforcer
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline
Mood: Ichthyoidal
|
|
There was a thread a long time ago about storing sulphuric acid in plastic bottles. Someone had tried it, and the bottle dissolved! Unfortunately,
the forum software screwed the thread up, and I can't remember what the plastic was.
If you diluted the acid down to 84% concentration (i.e. to sulphuric acid monohydrate), it would probably be a lot more manageable.
Quote: | Why not use glass? Like huge 1L cookie/mayo jars or something. |
Glass jars are resistant to most chemicals, but unfortunately, the metal lids are not! Even if the lid was never in direct contact with the acid, I
expect that prolonged contact with the vapour would severely corrode it.
1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
|
|
chemoleo
Biochemicus Energeticus
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
The H2SO4 I have was 96%, obtained OTC. They were stored in polypropylene bottles.
Over 2 years or so, the acid turned black, even though (thankfully) the bottles didnt dissolve.
Thinking, maybe PE is better - but it wasn't. The acid continued getting blacker.
Then I went to the local pharmacy and bought brown glass chemical bottles. They at last solved the problem. No cyrstals forming around the lid (in
fact, the lid, after 3 years of exposure, is absolutely untouched - made of PP), and the glass didnt get milky on the outside.
Since then that's the container of choice, for such acids.
For HNO3 >90% I use glass stoppered bottles only.
Obviously you can't ever use metal lids, even if they are covered by some sort of plastic. After a few years they will be eaten through
nonetheless.
I should mention that I still use the black H2SO4, I reckon it's just fine carbon.
Never had a problem with it either.
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
Organikum
resurrected
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2336
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
HDPE should be just fine. My 98% H2SO4 (66 Bé) comes in such bottles. Yes the acid darkens by time, but as told this does by no way affect its
usability.
I am not sure on this, but I think that high concentrated H2SO4 is less prone to eat plastics than H2SO4 in concentrations between 50% and 90% is -
but I may be wrong on this.
|
|
thunderfvck
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 347
Registered: 30-1-2004
Location: noitacoL
Member Is Offline
Mood: No Mood
|
|
WHat about wine jars? Those are nice, amber usually. I have a nice 4 L one that's just asking me to be filled with conc. H2SO4. Lid is plastic
(HDPE).
|
|
thalium
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 123
Registered: 2-11-2004
Location: Bottom of Hell
Member Is Offline
Mood:
|
|
About glass jars: you could try to use them with a glass lid...just a idea..
I don\'t believe in ghosts but they believe in me
![](http://img411.imageshack.us/img411/9620/userbar561032cr2.gif)
Hell was full so I came back..
|
|
I am a fish
undersea enforcer
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline
Mood: Ichthyoidal
|
|
Quote: | Originally posted by thalium
About glass jars: you could try to use them with a glass lid...just a idea.. |
...and these matching glass lids can be purchased from where exactly? The thread was about making use of readily available containers.
Your sarcasm would be slightly more tolerable if your name was spelt correctly.
1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
|
|
jimwig
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
there are "materials" oriented sites that list the physical and chemical properties of types of plastics, etc on the basis of resistance to
degradation thus making a decision as to which type to use somewhat informed.
|
|
thalium
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 123
Registered: 2-11-2004
Location: Bottom of Hell
Member Is Offline
Mood:
|
|
about my name...I don't like it anyway as it wasn't my idea and about the glass lid I just happend to see a jar like this at a local store
but I actually don't think it is of some use for this...you sholud be able to find proper storage bottles and jars at shops where they sell other
glassware
I don\'t believe in ghosts but they believe in me
![](http://img411.imageshack.us/img411/9620/userbar561032cr2.gif)
Hell was full so I came back..
|
|
thalium
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 123
Registered: 2-11-2004
Location: Bottom of Hell
Member Is Offline
Mood:
|
|
also about my name: when I made my yahoo! user I forgot to spell an L and I registered here with it because I'm not a fan of 5000 names
I don\'t believe in ghosts but they believe in me
![](http://img411.imageshack.us/img411/9620/userbar561032cr2.gif)
Hell was full so I came back..
|
|
mick
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 338
Registered: 3-10-2003
Member Is Offline
Mood: No Mood
|
|
It could be how much you use it. I have a 20+ year old bottle of 98% sulphuric acid ex BDH that I was going to de-rust car parts with using dibutyl
thiourea as the inhibitor. Never got round to it, but the sulphuric acid is still spotless. Amber glass winchester, pp top, not sure of the seal, and
kept in an outer black pp? container. The new stuff is in pp containers, they seem OK but as mentioned the acid gradually darkens. I have got some
bromine that has been sealed for over 18 months in glass with a silicone backed ptfe seal + pp top, it seems OK, the seal has darkened slightly but is
not brittle. Trying the same with conc nitic, 12 months OK.
mick
ptfe seals seem to be turning up regular, I found them in the top of cod liver oil bottles.
mick
[Edited on 4-11-2004 by mick]
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Here is a chemical resistance guide with different plastics and how well they work for different concentrations of sulfuric acid.
Apparently, PE is good up to 80*C.
Attachment: Chem resistance guide.pdf (19kB) This file has been downloaded 864 times
|
|
tom haggen
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline
Mood: a better mood
|
|
I wrote a similar thread about this same topic a few months ago. Although, my thread was about PETE. A simple Google searched yielded the information
that this plastic was incapable of storing strong acids. The reason I was inquiring about this in the first place is because when I would use HDPE for
storing strong acids I could never get a good seal between the container and the lid. The reason for this is because in a lot of OTC HDPE containers
the lids have these little Styrofoam like disks that keep an air tight seal. Of course those disks are not resistant to strong acid so I would always
take them out losing my air tight seal. So eventually I just found a good HDPE container, and left the little disk up in the lid. As long as no acid
splashes up on the lid there really isn't any problem. I've had my 90% H2SO4 in a HDPE container for months now, and although it appears to
be a darker color in the container, when you pour it out in small quantities in a glass container, the acid is actually quite clear. So to answer your
question HDPE is an excellent material for storing chemicals. Of course there are a few exceptions like conc. nitric acid, or hydrofluoric acid. The
problem lies with having a good seal at the lid. Since HDPE tends to be somewhat flexible it makes it difficult to get a good seal. If you don't
believe me, take a gallon of milk turn it upside down and squeeze that fucking thing like you are going to have a conniption if it doesn't
explode. You will notice that milk will leak out of the sides of the lid.
N/A
|
|