Boiling metals Copper and Aluminum
I tried to heat these metals in an electric arc to boil them.
And it succeeded ....
<iframe sandbox width="420" height="315" src="http://www.youtube.com/embed/ASvNnZWmiiA" frameborder="0" allowfullscreen></iframe>
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
It is not an good idee to boil metal , you can catch the metal fume fever.
I never asked for this.
|
|
Neil
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
Normally it is zinc which gives you fume fever. Copper gives you a case of coughing, hacking, sore throat and death. To be honest I can't recall what
boiling Al does to your lungs, other then it would be likely be Al2O3 by the time it made it to you, a nuance dust IIRC.
In ether case we hope your wearing the correct protection yadda yadda.
I'm missing the point of your latest posts, where's the mustard? er science? Or are you just experimenting to see what does what? Are you playing with
boiling point depression or alloys?
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Hmmm... these metals should condense quite quickly in the cold, surrounding air, subjecting the experimenter possibly to fine oxidised metal powder,
not to metal vapour. Zinc has the lowest BP though... A good quality dustmask is the least kind of protection needed, at a minimum, in all cases.
|
|
Neil
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
True, though the copper stays metallic for a while. CuO/Al will nicely Cu plate; grass, twigs, the inside of your lungs, acorns, plastics etc.
The copper is a toxic heavy metal irritant
Zinc oxide triggers a massive immune response (some times) - the fume fever is the result.
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
can you alloy both metals?
|
|
Neil
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
aluminium bronze.
|
|
neptunium
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 987
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline
|
|
Al boil at 2740 K ....impressive ...although an arc welder can reach 10 000 F a TIG can get it up to 35 000 F ! Al is easy target..try tungsten at
5930 K !! have fun!
|
|