Pages:
1
2 |
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
If I had the money to buy CsNO3 I'd simply buy CsCl and circumvent all this chemical juggling, to be honest!
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Incidentally, what do biochemistry labs do with the CsCl after they use it?
I'm thinking a bit of drying down then roasting to degrade organics followed by a recrystallisation would get me CsCl almost for free.
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
The problem is that I don't have money to buy CsCl, only CsNO3 from a handy Russian dealer that sells it surprisingly cheap (200g of CsNO3, 10-20 of
sodium metavanadate and 1g of luminol) for 34$ including shipping. The next best thing is companies as NYliquidation on eBay, the'r prices and purity
is good, but the shipping price is ridiculously high (35-55 if I remember correctly, and just for a 200g package).
Also, I find the chemical juggling quite fun (at least for the first time of each type of juggling).
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
The juggling is what we're here for but if e.g. you wanted CsOH (for reduction with Mg/t-butanol) then the additional step of converting CsNO3 to CsCl
is just a pain.
Watch for a U2U.
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
Actually I would prefer CsOH over CsCl, because it will be easier to transform it to CsBr/CsI for other experiments (HI/HBr is quite costly). Can you
give me a brief explanation of the process of converting CsNO3 to CsOH (note that I don't have access to high temperatures)?
[Edited on 10-10-2011 by Mixell]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
I believe CsOH is prepared the same way as most alkali hydroxides: electrolysis of a Cs salt in controlled conditions, followed by contration of the
CsOH solution. Yum, yum!
For small quantities this displacement can be used: Cs2CO3(aq, s) + Ca(OH)2(sq, s) === > 2 CsOH(aq) + CaCO3(s) which exploits the great
insolubility of CaCO3. KOH can be made this way. But you're still left with concentrating the most caustic of all hydroxides!
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
What kind of electrodes and voltage will one need to perform such an electrolysis? I assume something in the direction of MMO coated titanium? Cs2CO3
would be nice too, may be even better then CsOH (less caustic).
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
At the moment you have the option of buying CsOH if you live in Europe. I just purchased 20 grams of this and will try the making of Cs-metal from
this.
http://www.ebay.co.uk/itm/CESIUM-HYDROXIDE-10g-/280748109872...
It is not really cheap, but it is quite affordable. I hope to be able to make a few grams of Cs-metal from this.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Fantastic, woelen. How will you try and make the metal? Prometheus?
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I'll try the same method as with making potassium, based on POK's procedure. First I'll try on a very small scale, due to the dangerous nature of
Cs-metal. I'll also test wether glass can be used for this experiment. I have read lots of nasty stories about the ease at which CsOH attacks glass. I
expect that it will not differ much from NaOH or KOH in this, but before I make a lot of Cs I have to be sure that no accidents happen.
Now I am waiting for the CsOH to arrive... it probably takes 1 to 2 weeks, based on previous experience with the same seller.
[Edited on 11-10-11 by woelen]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Woelen:
If I recall well the patented method differs somewhat for caesium (starts from the Cs butoxide), so please refresh memory. Look forward to your
trailblazing effort!
I can’t see CsOH being much more aggressive to glass than KOH, assuming we’re below MP.
And NOW look what you’ve made me go and do: buy some CsOH too (10 g)! Sheesh… life’s not fair…
[Edited on 11-10-2011 by blogfast25]
Also woelen, considering how dangerous Cs metal is, I'd be prepared well to ampoule any metal obtained. I've got some nice mini glass bulb pipettes
(1, 2 ml and less too), if you're interested...![:cool:](./images/smilies/cool.gif)
[Edited on 11-10-2011 by blogfast25]
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Good to read that you also purchased some of the CsOH. I'm quite sure it can be used for many interesting experiments. In my first attempt I indeed
think of making 1 gram or so and then a 2 ml ampoule would be nice. How do these ampoules look like?
When the CsOH arrives, then I'll first try the experiment on a test tube scale and if this gives promising (and safe) results, then I'll scale up.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by woelen ![](images/xpblue/lastpost.gif) | How do these ampoules look like?
When the CsOH arrives, then I'll first try the experiment on a test tube scale and if this gives promising (and safe) results, then I'll scale up.
|
I would use a small bulb pipette, 1 or 2 ml depending on scale:
http://www.google.co.uk/imgres?imgurl=http://www.eloh.com.sg...
I've quite a few to spare, if you're interested.
Warm slightly, suck up (using pipette pear) some kerosene, then some molten metal, then some more kerosene, thereby trapping the metal between 2
layers of inert solvent, allow to cool. It should reveal the slightly golden hue of the metal. Practice with your K stockpile first!
|
|
Pages:
1
2 |