Ts joint sizes


I've been trying to find a conversion table for Ts joints. I want to get some 29/42 glass stoppers but the site only gives numbers, e.g., "No. 27". I would have thought that this information would be easy to find but I've been searching quite a bit and haven't yet found it.

Thanks for any help.
View user's profile View All Posts By User
Neil
National Hazard
****




Posts: 556
Registered: 19-3-2008
Member Is Offline

Mood: No Mood

[*] posted on 25-9-2011 at 03:55


Is the joint you are trying to stopper standard taper?

If so you need to find a standard taper 29/42 stopper which is a size that occasionally comes up on Ebay.

the numbered sizes use a different taper and will not fit to a standard taper joint.

http://what-when-how.com/organic-chemistry-laboratory-surviv...


Glass joint sizes

http://www.wilmad-labglass.com/pdf/taper_ground_joint_dims.p...

View user's profile View All Posts By User
mr.crow
National Hazard
****




Posts: 884
Registered: 9-9-2009
Location: Canada
Member Is Offline

Mood: 0xFF

[*] posted on 26-9-2011 at 10:18


The numbered joints are used for things like volumetric flasks and sep funnels. The other ST joints are for glassware.

24/40 is the most common, but 29/42 is good for larger flasks. Get a reducing adapter, very useful.




Double, double toil and trouble; Fire burn, and caldron bubble
View user's profile View All Posts By User
ScienceHideout
Hazard to Others
***




Posts: 391
Registered: 12-3-2011
Location: In the Source
Member Is Offline

Mood: High Spin

[*] posted on 26-9-2011 at 12:28


I reccoment ST 19/22. Love it!



hey, if you are reading this, I can't U2U, but you are always welcome to send me an email!


View user's profile Visit user's homepage View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 26-9-2011 at 12:32


I have a few 29/42 glass stoppers, how many are you looking for? I could sell you a few for about $2 each plus shipping.

And I agree with Neil that a glass stopper with a single number will not fit correctly. There are probably a few people selling them on Ebay as well, but it is a less common size that 24/40, 19/22 or 14/20.

Bob

View user's profile View All Posts By User
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 27-9-2011 at 05:23


As usual, there is an European ISO standard and an US standard (what idiot came up with the idea to make 2 standards?), but they can usually be used together and differ in the length of the taper only.

The other number can be simply ignored for most applications, except when you're trying to do something really important and you've got a box full of both standards. But that's happens almost never.
Because of that, and the fact my glassware is all European ISO, I use the typical "NBxx" notation, where NB means the same thing as NS in German language - nominal bore or normal bore, or normal schliff kern if I'm correct.

NB19 is a very good one and AFAIK the most common of all at college laboratories. Other than that, NB14, NB24 and NB29 are used. Other tapers are rare. 14, 19 and 24 are the best ones for home experiments, though NB14 is usually reserved for thermometers and alike.
I've got some NB29 flasks so a reducing adapter would be handy. Luckily, I know a good flameworker that does his job well so that won't be a problem. Except for the money. Money is always a problem. :D

Does anyone of you have any experience with those barb protrusions used to mount steel springs? They seem to be a much cheaper option instead of Keck clips, but I'm not sure if clips can be mounted on a joint supplied with barbs.

[Edited on 27-9-2011 by Endimion17]




View user's profile Visit user's homepage View All Posts By User
Mildronate
Hazard to Others
***




Posts: 428
Registered: 12-9-2009
Member Is Offline

Mood: Ruido sintetico

[*] posted on 27-9-2011 at 22:06


I use 14 and 29, 19 and 45 rare. My favorite is 29 :)
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 28-9-2011 at 09:50


Quote: Originally posted by Endimion17  

Does anyone of you have any experience with those barb protrusions used to mount steel springs? They seem to be a much cheaper option instead of Keck clips, but I'm not sure if clips can be mounted on a joint supplied with barbs.


I have used the glassware with barbs and haven't found that to be the best solution for several reasons:

1) the barbs break off easily and leave sharp edges that cut you

2) the springs are small and easily lost, my fingers are clumsy

3) you cannot rotate joints easily with barbs

4) barbed glassware cost more

5) keck clamps give before apparatus blows up in the case of overpressurization.

6) Keck clamps and steel clips are cheap in the long run.

Bob
View user's profile View All Posts By User
jock88
National Hazard
****




Posts: 505
Registered: 13-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 17-10-2013 at 12:52



What are the advantages and disadvantages of different joint sizes in combination with different vessel sizes. I find the joint sizes baffling.

See here
http://www.ebay.co.uk/itm/NEW-Large-20L-20000ML-45-40-Round-...

and here
http://www.ebay.co.uk/itm/20ML-Round-bottom-boiling-flask-29...

Last link is an extreme example of a small vessel with a large joint.


What size is used for what. Is there a discussion/writeup somewhere on the net about this?
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2013 at 12:09


Large joint flask are normally used where one wants to stir with a mechanical paddle stirrer, and the better ones are too big to fit through a 24/40 jointed neck on a flask. There are also other reasons to use them for larger flasks, just due to the larger area, which allows faster distillations, etc, as vapor flow is proportional to diameter of the neck.

On a separate note: People still need to understand that a ST22 or ST 27 glass stopper size and taper angle is NOT the same as the 14/20, 19/22, 24/40, or 29/42 type joints on flasks and other items. So a TS#14 stopper will NOT fit into a 14/20 joint, and a TS#19 stopper will not work in a 19/22 joint, etc. So please be careful when describing the stopper or joint size to use both numbers if they are there.

But with two number type sized joints, all joints of the same first number have the same taper, and will fit into each other, thus a 19/22 male end will fit into a 19/38 female joint just fine, just not reach all the way in.