Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Extracting lead and tin from solder.
TriiodideFrog
Hazard to Others
***




Posts: 108
Registered: 27-9-2020
Member Is Offline


[*] posted on 6-1-2021 at 23:53
Extracting lead and tin from solder.


Does anyone know how to extract lead and tin from solder? Maybe using copper acetate to dissolve the lead? Thanks in advance.
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

[*] posted on 7-1-2021 at 00:27


NO! don't even think about it. it's one thing to handle solder and death wish to play with PB solutions. just get Tin from pewter.
..




"A mind is a terrible thing to lose"-Meisner
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3692
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 7-1-2021 at 00:36


modern pewter is mostly tin, with a few percent copper, antimony and/or other,
but original/antique pewter contained about 30% lead,
so check before using.
99.9% tin ingots are not too expensive via eBay etc.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 7-1-2021 at 00:51


Some good ideas in here http://www.sciencemadness.org/talk/viewthread.php?tid=2277
View user's profile View All Posts By User
highpower48
Hazard to Self
**




Posts: 98
Registered: 30-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 7-1-2021 at 09:53


How about removing the 1% silver from lead free solder, which is 99% tin and 1% silver.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3032
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 7-1-2021 at 10:08


Quote: Originally posted by rockyit98  
NO! don't even think about it. it's one thing to handle solder and death wish to play with PB solutions. just get Tin from pewter.
..


Don't eat Pb solutions and don't breath the aerosols, you will be fine.

You can easily buy 60/40 Sn/Pb solder, when you dissolve this in nitric acid you get lead nitrate and SnO2. The nitrate will be dissolved and the oxide will be a white solid which you can filter.
View user's profile View All Posts By User
TriiodideFrog
Hazard to Others
***




Posts: 108
Registered: 27-9-2020
Member Is Offline


[*] posted on 8-1-2021 at 03:17


Ok, thanks! Maybe I will just get pewter.
View user's profile View All Posts By User

  Go To Top