Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: remagnetize a demagnetized magnetic stir bar
rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

shocked.gif posted on 26-11-2020 at 07:28
remagnetize a demagnetized magnetic stir bar


i was making 98% H2SO4 and i forgot one of my magnetic stir bars in the vasal. so it got hotter than rated 250C and became a dud. even before that it was getting weaker by repeated use.

then I remembered watching a "how it's made" episode where they showed how magnets are made.in it by pulsing the pre magnetize "magnet" with a strong magnetic field it becomes a magnets. it's due to a process called " Magnetic hysteresis ".with this knowledge i made a simple yet effective way to remagnetize such stir bar.

WARNING- RISK OF ELECTRIC SHOCK
do this away from sensitive electronics
repeat at your own risk
using magnet wire i wound a coil with a bobbin that match the stir bar so it will side right in easy. about 100 turns (i forgot to count :D)
i used 330uF 400V Electrolytic capacitor (mind the polarity ) charged up to 325V using AC mains by using full bridge rectifier and a incandescent light bulb. after charging the capacitor while being careful I removed it.
after i inserted the stir bar inside i fix it at the center and parallel with the coil with a dab of hot glue. after it's secured in place i shorten the capacitors terminals with the coil. with that tiny sparks flew and it was done.it was better than new!
NOTE : important
remember to strip the enamel at the tips of the magnet wire
use rubber gloves and eye protection , double check polarity otherwise capacitor will explode, use rated 400V or higher capacitor


cap.jpg - 101kB coil2 .jpg - 189kB cap2.jpg - 162kB fbr..jpg - 138kB CHARGING.jpg - 31kB discharging.jpg - 19kB coil.jpg - 278kB




"A mind is a terrible thing to lose"-Meisner
View user's profile View All Posts By User
VeritasC&E
Hazard to Others
***




Posts: 176
Registered: 29-1-2018
Member Is Offline

Mood: No Mood

[*] posted on 31-7-2022 at 01:43



What is the influence of temperature on this?

One one side maybe a stir bar remagnetizes in a lower magnetic field when initially at a higher temperature (as long as the max temperature reached during the process stays sufficiently below its curie temperature).

One the other side, while a colder stir bar maybe would require a greater magnetic field to achieve equal magnetization, it is possible that more magnetic domains would remain in their "magnetized" state after the process, and thus, that a greater degree or magnetization can be achieved this way (especially since the process probably increases the temperature of the stir bar while magnetizing it).

It would be interesting to measure the temperature difference induced during (re)magnetization, and to try to accordingly cool it down just as much as necessary for its maximum temperature during the process to stay under, say, 10C. Whether that requires a freezer or a nitrogen bath is a good question.

Note that this is all based on assumptions from my part. I am not sure that this is scientifically correct.

In any case, thank you for this post which certainly will be useful for many (including myself). I'll be much more relaxed about the conditions in which I opt for magnetic stirring when I have the capacity to remagnetize my stir bars.
View user's profile View All Posts By User