Keeping Ammonium fluoride solution in a glass bottle


I have 500g of ammonium fluoride NH4F powder that I use to make metal fluorides by double displacement. But I hate working with the powder it seems to sublimate very quickly. Thus I want to keep some as a solution, probably 150g dissolved in 200ml water.
My question is, can I keep this solution over a long period of time in a glass thick wall reagents bottle? I read the ammonium fluoride solution will etch glass, but I don’t know if this is something to be concerned about.
Advice will be appreciated, I know near nothing of fluorine compounds.

[Edited on 3-6-2020 by Lion850]
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 3-6-2020 at 01:33


Why not just use a plastic bottle?
View user's profile View All Posts By User
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 3-6-2020 at 02:12


I happen to have a few spare glass reagent bottles. But if necessary I’ll get a plastic one. I’m still interested to understand how long a glass bottle will last.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3692
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 3-6-2020 at 03:14


Earlier today I was browsing and came across something that could be ideal,
ptfe coated hdpe bottles https://www.lazada.com.my/products/ptfe-bottle-food-grade-wi...
probably available via ebay, amazon etc. - I've not looked




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 3-6-2020 at 05:03


https://www.youtube.com/watch?v=LRw5-WQERbM

there's a reason if it is used to etch glass, because it etches glass. use a plastic container





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 3-6-2020 at 09:44


Quote: Originally posted by Ubya  
https://www.youtube.com/watch?v=LRw5-WQERbM

there's a reason if it is used to etch glass, because it etches glass. use a plastic container


That's ammonium bifluoride, i.e. NH4F . HF
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 3-6-2020 at 10:08


Quote: Originally posted by DavidJR  
Quote: Originally posted by Ubya  
https://www.youtube.com/watch?v=LRw5-WQERbM

there's a reason if it is used to etch glass, because it etches glass. use a plastic container


That's ammonium bifluoride, i.e. NH4F . HF


yup bifluoride is the one commonly used to etch glass, but after checking again ammonium fluoride also is corrosive against glass, slower than the bifluoride, but still corrosive.





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------