Cerium pyrophoricity
Hi.
I am thinking about buying some cerium metal. I read some time ago that cerium is pyrophoric. I suppose that only in form of dust, but I am not sure
about that. Have you some experiences with storing cerium metal?
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
In finely divided form, it's pyrophoric. See this page for behavior in bulk form:
https://www.elementsales.com/re_exp/
Under argon or mineral oil, it should present no significant problems.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 514
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Ferrocerium rods contain a large percent of cerium, and those don't catch fire spontaneously. You will be fine.
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Thanks.
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Hi.
I finally have cerium metal . I bought it along with Mo and Mg powders. Seller
send it in plastic vial with mineral oil. 3g of Ce costs 117Kč (4,25€).
For CZ members: I bought these metals here. This seller mainly sell elements - for hobby chemists and also for element collectors. He also sells some chemical compounds and other
useful stuff.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
I've had Cerium lumps. It oxidizes fast and disintegrates as a powder.
Never tried to use it in a composition and see if there was metal left or just the oxide.
Storing in oil seems smart.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
Fery
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1009
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline
|
|
Bedlasky - do you need Ce metal, couldn't you use its oxide which is much more cheaper?
I visited the eshop you mentioned few times already but always found cheaper sellers, especially from Poland where no problem of buying few kg which
were on stock and shipped immediately.
|
|