Nickel carbonate!
Hello!
Some days ago i've synthetized nickel carbonate. I do it in two steps: first, i make react metallic nickel and copper sulfate solution. After some
hour the solution from light blue becomes transparent and copper settles in his surface (nichel sulfate in solution). I filter the solution from
copper powder, then i add sodium carbonate to the solution and dark green precipitate forms . Now, i tried this process to make others metals
carbonate. I placed some lead piece in the CuSO4 solution, but no reaction is visible. Do lead (slowly) react? And tin? Tin should react with copper
sulfate, so tin carbonate is a possible synthesis (maybe). Is this process right? Which metals react with CuSO4?
Thanks
|
|
Fery
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline
|
|
Look for metal redox potential table. Pb is very close to Cu so reacts very slowly. Additionally, the Pb surface in CuSO4 is covered with PbSO4 which
is poorly soluble in water and almost insoluble especially in a solution containing significant concentration of sulfate anions (due to CuSO4).
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
Dipping iron in cuso4 plates copper onto the iron and leaves iron sulfate in solution.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
The problem is the formation of insoluble lead sulfate, as Fery says.
I've tried it with copper acetate, and that works fine. It's slow, but it works.
-----