Member Is Offline
|
|
Chromium nitrate from Cr2O3 + HNO3?
I need some Chromium nitrate to create copper chromite using a sol-gel process.
Its seems to be expensive to buy. Can I make chromium nitrate by disolving chromium oxide in 70% HNO3?
If so, do I simply dry the resulting solution and wash?
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 771
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Quote: Originally posted by jderimig ![](images/xpblue/lastpost.gif) | I need some Chromium nitrate to create copper chromite using a sol-gel process.
Its seems to be expensive to buy. Can I make chromium nitrate by dissolving chromium oxide in 70% HNO3?
If so, do I simply dry the resulting solution and wash? |
Probably not unless your oxide is freshly precipitated. I have a flask containing pottery grade oxide in sulphuric acid. After months none has
dissolved judging by the colour. Apparently you have to digest it in molten alkali first. Do a search you will find a detailed procedure.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
jderimig
Harmless
Posts: 10
Registered: 25-11-2019
Member Is Offline
|
|
A little more research says Chromium Nitrate can be produced from Chromium Trioxide, CrO3, and nitric acid. I haven't found any CrO3 that is cheaper
than Chromium Nitrate...
So I guess I will just open my wallet....