Why can't I dissolve my CuI in acetonitrile?
Hello chemist friends.
I made some copper iodide by adding solution of potassium iodide to a solution of copper sulfate in 1:1 stoichiometric ratio. I filtered and washed
the precipitate with water and then with ethanol to dissolve all elemental iodine that formed. I then let it thoroughly dry out outside. The product
is completely insoluble in water and alcohol.
I wanted to make crystals and sources (wiki, researchgate) suggest it should be 7-8% soluble in acetonitrile.
However, I couldn't even get 0.5g of it dissolved in 50g of boiling acetonitrile. What could be the problem here? After filtering the acetonitrile
"solution" no crystals or precipitate formed on cooling down.
My acetonitrile is pure and from a chem supplier.
Attached is a photo of my supposed CuI.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
I wonder if it started photodecomposing like silver iodide would. It should be white.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
it should be white if pure, but most samples have an off white color as copper iodide easily adsorbs free iodine from the solution it was made from, a
simple washing may be not enough.
as to why it didn't dissolve in acetonitrile could it be because the solvent was wet?
if it is so insoluble in water i assume that adding water to a solution of AcCN and CuI would crash it out of solution pretty quickly.
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Did you try adding CuI to MeCN in very small increments, ie only a few grains of the powder? That way you can see if it's really that insoluble.
[Edited on 191120 by fusso]
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Was the solution from which you made CuI neutral or acidic. I also made CuI once, but this worked best when the solution was a little acidic.
Otherwise I obtained a brown/orange impurity, which I could not separate from the CuI and which did not disappear on adding a reductor like Na2SO3. I
think that the brown impurity is Cu2O or a hydrated variation of that.
I made my CuI by adding a copper sulfate solution to a solution of KI (I used approximately stoichiometric amounts, one KI for one CuSO4.5H2O, with a
little excess KI). I added an acidified solution of Na2SO3 to this. This works as a reductor. I dissolved the KI and acidified Na2SO3 in water
(giving a pale yellow solution, due to coordination of I(-) and SO2) and dissolved the CuSO4 in another amount of water, and then mixed the solutions.
An off-white precipitate is formed. Do not add too much Na2SO3! My material is not white, but it is greyish-tan, not reddish-brown like yours. I used
it in an experiment with pyridine, making a fluorescent complex. I did not dry it, I just filtered it and rinsed with water and then stored under
water. CuI, especially when humid, is air-sensitive, and is easily oxidized by oxygen from air.
|
|
Fery
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline
|
|
How does the solubility curve look like? There are systems where the solubility of a solid in a solvent does not change too much according temperature
e.g. NaCl - H2O. There are even systems where solubility decreases as temperature increases (inverted solubility curve) e.g. CaSO4 - H2O, MnSO4 - H2O,
Ce2(SO4)3 - H2O. Perhaps the some could exist for organic solvents, not only for H2O.
Cu(I) binds with acetonitrile into a complex (also with pyridine as woelen pointed out). I believe even if you are able to obtaining crystals from
acetonitrile solution they won't be CuI anymore but a complex (and this complex could be very soluble in acetonitrile). Did you try to distill out the
solvent after you did not obtain crystals on cooling down?
For a crystallization it could be helpful to introduce crystal seeds or at least scratch walls of supersaturated solution. Decades ago when I
crystallized abietic acid it last few weeks, the system had consistency of honey, few days latency when no crystals, then the amount of crystals
increased very slowly every day.
|
|
Fery
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline
|
|
and here some experiments how to grow CuI crystals and discussion about their discoloration - they used NH4I aqueous solution
https://sci-hub.tw/https://pubs.acs.org/doi/pdf/10.1021/acs....
https://sci-hub.tw/https://aip.scitation.org/doi/10.1063/1.5...
|
|
rockyit98
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline
Mood: no mood is a good mood
|
|
Quote: Originally posted by michalJenco ![](images/xpblue/lastpost.gif) | Hello chemist friends.
I made some copper iodide by adding solution of potassium iodide to a solution of copper sulfate in 1:1 stoichiometric ratio.
|
dude! watch your chemistry.the ratio is 2:1 ( 4KI +2CuSO4 -------->Cu2I2 +I2 +2K2SO4)
Cu2I2 (Copper(1+)diiodide) is CuI but written differently.
if it helps, i made pure CuCl (Cu2Cl2) by passing a current through a Con. NaCl solution by using Cu wire which are 99.9% pure. 2NaCl + 2Cu +H2O
------> Cu2Cl2 +2NaOH +H2) i think KI might do better given Cu2I2 has much lower solubility.
"A mind is a terrible thing to lose"-Meisner
|
|
mayko
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1218
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
Another possibility might be to dissolve the CuI in an aqueous iodide solution and then diffuse through an iodide-free gel, with crystallization
taking place when the complexing agent drops in concentration. There's a mention of this technique as applied to cuprous chloride here:
https://www.sciencemadness.org/whisper/viewthread.php?tid=75...
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Depends . . .
If you add a suitable reductor, you can use all iodine for binding to Cu and then you can indeed use a 1 : 1 ratio. I did that in my experiments with
formation of CuI-pyridine complexes. Iodine/iodide is relatively expensive, while Na2SO3 (the reductor) is dirt cheap.
|
|
michalJenco
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 50
Registered: 7-2-2019
Member Is Offline
|
|
Wow, thanks for all the responses! I will answer some of your questions and give you updates.
My solvent is not wet, label says <2% H2O.
Adding water to the filtered acetonitrile "solution" really did give a white precipitate, it was even crystalline (tiny flakes which reflected light).
I needed to add about the same volume of water to make it crash out, however, not just a tiny bit. I heated this new solution with precipitate to
almost boiling and even added about 50% further acetonitrile, but it didn't all dissolve back. Right now I am waiting for the filtrate to cool down
and maybe crystallise out whatever re-dissolved.
I figure some of the CuI I made really decomposed into an insoluble oxide and I didn't judge correctly whether anything dissolved at all.
I didn't add any acid when originally making the CuI, just CuSO4.5H2O and KI. Apparently it worked anyway. But thanks for your experimental
experience, woelen.
I did not try to distill the solvent after the precipitate did not form. I did scratch the glass beaker with a glass rod and introduced seeds of the
crude CuI, however. Didn't do anything.
|
|
michalJenco
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 50
Registered: 7-2-2019
Member Is Offline
|
|
Quote: Originally posted by woelen ![](images/xpblue/lastpost.gif) |
Depends . . .
If you add a suitable reductor, you can use all iodine for binding to Cu and then you can indeed use a 1 : 1 ratio. I did that in my experiments with
formation of CuI-pyridine complexes. Iodine/iodide is relatively expensive, while Na2SO3 (the reductor) is dirt cheap. |
So that is why so much elemental iodine was formed in my synthesis .. next time I will use Na2SO3 as a reductor and see how I2 formation reduces!
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Exactly, and that also is the reason why I added some acid, because Na2SO3 is somewhat alkaline and without acid you get all kinds of side reactions,
with formation of oxides and hydroxides. As an alternative, you could add sodium metabisulfite instead of sodium sulfite. Just be sure that the
solution remains on the acidic side of the pH-scale.
|
|