Dehydratation of FeO(OH) and CaSO4


Hello.

I had some hydrated ferric oxide and calcium sulphate dihydrate from experiments I've made long ago. So I decided to dehydrated them in oven at 275°C. But I am little confused from result of this dehydration.

CaSO4 isn't white but beige. Is this normal or is it contaminated by some organic impurities?

Ferric oxide isn't red but black. Why?

IMG_20190424_191743.jpg - 1.8MBIMG_20190424_191724.jpg - 1.8MB
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 24-4-2019 at 21:50


Try magnet test. If it's attracted to magnet it's Fe3O4.



View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 25-4-2019 at 01:09


most ferric oxide produced with wet chemistry is black. look at nurdrage's video on the preparation of ferric oxide for thermite, he uses 3 methods, and only the electrolytic one gives red iron oxide




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1227
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 30-4-2019 at 18:52


Quote: Originally posted by fusso  
Try magnet test. If it's attracted to magnet it's Fe3O4.


I tried this and it had not attracted to magnet.

Quote: Originally posted by Ubya  
most ferric oxide produced with wet chemistry is black. look at nurdrage's video on the preparation of ferric oxide for thermite, he uses 3 methods, and only the electrolytic one gives red iron oxide


Thanks!
View user's profile View All Posts By User
CharlieA
National Hazard
****




Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline

Mood: No Mood

[*] posted on 1-5-2019 at 16:14


Am I correct in assuming that Fe3O4 is a typo? Or is this FeO(dot)Fe2O3. I am not familiar with this substance.
View user's profile View All Posts By User
oberkarteufel
Harmless
*




Posts: 47
Registered: 11-12-2018
Member Is Offline

Mood: Mayonesium sulfate

[*] posted on 1-5-2019 at 23:55


No, it's not a typo. This compound contains iron on both +III and +II oxidation states. There's also an oxide Pb3O4 with +II and +IV lead atoms.

Edit: Naturally occuring Fe3O4 is known as magnetite.

[Edited on 2-5-2019 by oberkarteufel]
View user's profile View All Posts By User
CharlieA
National Hazard
****




Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline

Mood: No Mood

[*] posted on 2-5-2019 at 17:18


Quote: Originally posted by oberkarteufel  
No, it's not a typo. This compound contains iron on both +III and +II oxidation states. There's also an oxide Pb3O4 with +II and +IV lead atoms.

Edit: Naturally occuring Fe3O4 is known as magnetite.


Thank you. I have learned something and that is a good think:)
Charlie A
View user's profile View All Posts By User