Random
International Hazard
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
Cerium salts from lighter flint
Is there a way to get cerium salts from lighter flint? It contains like 50% cerium along with iron and some other rare earths.
|
|
ScienceSquirrel
International Hazard
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
It is possible.
There are better and cheaper sources of cerium but if you want to do it as an exercise then go for it.
You want to dissolve 5g of the basic Misch metal as lighter flints in acid.
Take out the iron, leaving just cerium and the other lanthanides if they have not already been extracted by the processors.
Take out the cerium and you will be left with a solution containing small amounts of the other lanthanides.
|
|
ScienceSquirrel
International Hazard
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
You would be best off starting from ferrocerium rod rather than lighter flints as it is far cheaper.
Cerium is relatively easily separated from the iron, magnesium, lanthanum, etc as it can be take to CeIV and separated that way.
|
|
Xenoid
National Hazard
Posts: 775
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline
Mood: Comfortably Numb
|
|
This is discussed at some length in the following thread;
http://www.sciencemadness.org/talk/viewthread.php?tid=8758
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
An expensive source of cerium, methinks. Why not get some CeO2? Hard to dissolve but cheap as chips...
|
|
Random
International Hazard
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I will try dissolving them in acid and getting out iron. Thanks for the suggestions.
CeO2 is not available where I live.
|
|
watson.fawkes
International Hazard
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Cerium oxide is used as a polishing compound. Many sources of industrial
abrasives carry it for auto finishing, lapidary, machine lapping, etc.
|
|
arsphenamine
Hazard to Others
Posts: 236
Registered: 12-8-2010
Location: I smell horses, Maryland, USA
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Random | Is there a way to get cerium salts from lighter flint? It contains like 50% cerium along with iron and some other rare earths. |
Before 1950, hundreds of graduate chemistry degrees were earned by
the fractional crystallization of lanthanide salts. It was an incremental
purification process because there was no other way at the time.
Your job is easier since misch metal is already ~50% cerium.
Ce02 can be used as a feedstock, and powder can be got at Amazon cheaply ~$15/lb.
I read that the element is industrially electrolyzed from its chloride in a NaCl melt.
Benchtop production by thermal decarboxylation of the oxalate looks facile.
Since the metal is pyrophoric and somewhat toxic, reasonable precautions apply.
|
|