I am planing to do some etching test on metal sheet. I work at university so safety is number one. I have used HF before with other organics
solvents. Now I am planing to use glycerin and HF mixture. Before i do that i want to know what will happen if these two mix. I apperciate your
help. thank you.
|
|
merrlin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 110
Registered: 3-4-2009
Member Is Offline
Mood: No Mood
|
|
I have used glycerine/HF/nitric mixtures for metallographic etching with good results. In general, I like to avoid HF, but there are some applications
in which it gives the best results. HF deserves the utmost respect. Skin contact can result in absorption that leads to bone damage, and it doesn't
always give that burning sensation on contact (see attached .mht file). If you specify a particular alloy, I can suggest an etchant composition.